US 10529554
Method for forming silicon nitride film selectively on sidewalls or flat surfaces of trenches
Granted 2020-01-07 · Filed 2017-05-11 · Application 15/592,730 · Utility · Kind B2 · Prior publication US 2017/0250068 A1, 2017-08-31
- Assignee as printed
- ASM IP Holding B.V., Almere (NL)
- Inventors
- Dai Ishikawa, Ome (JP); Atsuki Fukazawa, Tama (JP); Eiichiro Shiba, Tama (JP); Shinya Ueda, Hachioji (JP); Taishi Ebisudani, Tama (JP); SeungJu Chun, Anmyeon-eup (KR); YongMin Yoo, Seoul (KR); YoonKi Min, Seoul (KR); Seyong Kim, Daejeon (KR); JongWan Choi, Seojong-myeon (KR)
- CPC, current
- H01L21/0217; H10P14/69433; H01L21/02211; H01L21/02274; H01L21/0228; H01L21/0234; H01L21/31111; H10P14/6336; H10P14/6339; H10P14/6532; H10P14/6682; H10P50/283; H01J2237/3347
Abstract
A method for fabricating a layer structure in a trench includes: simultaneously forming a dielectric film containing a Si—N bond on an upper surface, and a bottom surface and sidewalls of the trench, wherein a top/bottom portion of the film formed on the upper surface and the bottom surface and a sidewall portion of the film formed on the sidewalls are given different chemical resistance properties by bombardment of a plasma excited by applying voltage between two electrodes between which the substrate is place in parallel to the two electrodes; and substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the film by wet etching which removes the one of the top/bottom portion and the sidewall portion of the film more predominantly than the other according to the different chemical resistance properties.
The claims as the USPTO long-text file prints them (text data version 20261117.3), split by PatentRef's claim parser (structure version 2): each claim's opening words, then one row for each element with its character offsets in the claim text, and the dependent claims under the claim they refer to. The split describes the text; it is not a reading of it. Each claim and each element has a link of its own. How the links are made.
Claim 1
Independent claim.
1. A method for fabricating a layer structure constituted by a dielectric film containing a Si—N bond in a trench formed in an upper surface of a substrate, comprising:
- Claim 1, element e1(i) simultaneously forming a dielectric film containing a Si—N bond on the upper surface and a bottom surface and sidewalls of the trench, 173–306
- Claim 1, element e2wherein a top/bottom portion of the dielectric film formed on the upper surface and the bottom surface and a sidewall portion of the dielectric film formed on the sidewalls are given different chemical resistance properties by bombardment of a plasma excited by applying voltage in a reaction space between two electrodes between which the substrate is placed in parallel to the two electrodes; 308–701
- Claim 1, element e3(ii) substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the dielectric film by etching which removes the one of the top/bottom portion and the sidewall portion of the dielectric film more predominantly than the other according to the different chemical resistance properties; and 708–1030
- Claim 1, element e4(iii) obtaining a reference plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, 1042–1248
- Claim 1, element e5wherein the plasma in step (i) is a capacitively coupled plasma (CCP) which is excited by applying RF power to one of the two electrodes, 1250–1386
- Claim 1, element e6wherein plasma density is higher than the reference plasma density, 1388–1454
- Claim 1, element e7wherein the etching in step (ii) removes the top/bottom portion of the dielectric film selectively relative to the sidewall portion of the dielectric film, 1456–1610
- Claim 1, element e8wherein obtaining the reference plasma density comprises performing the forming of dielectric films as recited in step (i), then determining the chemical resistance property by etching as recited in step (ii), then repeating these steps for a plurality of times using different plasma density values, then obtaining the reference plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, and wherein the dielectric film is a SiN film.1612–2173
5 dependent claims: 2 to 5 and 13 (2, 3, 4, 5, 13 on claim 1)
Claim 2
Depends on claim 1.
2. The method according to claim 1 , wherein
- Claim 2, element e1in step (i), the dielectric film is formed by plasma-enhanced atomic layer deposition (PEALD).45–138
Claim 3
Depends on claim 1.
3. The method according to claim 1 , wherein
- Claim 3, element e1the plasma is a plasma of Ar, N 2 , or O 2 .45–87
Claim 4
Depends on claim 1.
4. The method according to claim 1 , wherein
- Claim 4, element e1in step (i), a halogenated silane is used as a precursor.45–101
Claim 5
Depends on claim 1.
5. The method according to claim 1 , wherein
- Claim 5, element e1the etching is the wet etching, which is conducted using a solution of hydrogen fluoride (HF) or phosphoric acid.45–157
Claim 13
Depends on claim 1.
13. The method according to claim 1 , wherein
- Claim 13, element e1no annealing is conducted between steps (i) and (ii).46–98
Claim 6
Independent claim.
6. A method for fabricating a layer structure constituted by a dielectric film containing a Si—N bond in a trench formed in an upper surface of a substrate, comprising:
- Claim 6, element e1(i) simultaneously forming a dielectric film containing a Si—N bond on the upper surface and a bottom surface and sidewalls of the trench, 173–306
- Claim 6, element e2wherein a top/bottom portion of the dielectric film formed on the upper surface and the bottom surface and a sidewall portion of the dielectric film formed on the sidewalls are given different chemical resistance properties by bombardment of a plasma excited by applying voltage in a reaction space between two electrodes between which the substrate is placed in parallel to the two electrodes; 308–701
- Claim 6, element e3(ii) substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the dielectric film by etching which removes the one of the top/bottom portion and the sidewall portion of the dielectric film more predominantly than the other according to the different chemical resistance properties; and 708–1030
- Claim 6, element e4(iii) obtaining a reference plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, 1042–1248
- Claim 6, element e5wherein the plasma in step (i) is a capacitively coupled plasma (CCP) which is excited by applying RF power to one of the two electrodes, 1250–1386
- Claim 6, element e6wherein plasma density is higher than the reference plasma density, 1388–1454
- Claim 6, element e7wherein the etching in step (ii) removes the top/bottom portion of the dielectric film selectively relative to the sidewall portion of the dielectric film, 1456–1610
- Claim 6, element e8wherein obtaining the reference plasma density comprises performing the forming of dielectric films as recited in step (i), then determining the chemical resistance property by etching as recited in step (ii), then repeating these steps for a plurality of times using different plasma density values, then obtaining the reference plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, 1612–2126
- Claim 6, element e9wherein the plasma density is modulated by tuning the pressure in the reaction space, 2128–2212
- Claim 6, element e10wherein the plasma density increases by lowering the pressure.2214–2275
2 dependent claims: 7 and 8 (7, 8 on claim 6)
Claim 7
Depends on claim 6.
7. The method according to claim 6 , further comprising,
- Claim 7, element e1prior to steps (i) and (ii), repeating the following steps to determine the reference plasma density: 57–157
- Claim 7, element e2simultaneously forming a dielectric film under the same conditions as in step (i) except that the pressure is changed as a variable; and 159–290
- Claim 7, element e3substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the dielectric film by etching under the same conditions as in step (ii).296–472
Claim 8
Depends on claim 6.
8. The method according to claim 6 , wherein
- Claim 8, element e1the pressure in step (i) is controlled below 300 Pa.45–96
Claim 9
Independent claim.
9. A method for fabricating a layer structure constituted by a dielectric film containing a Si—N bond in a trench formed in an upper surface of a substrate, comprising:
- Claim 9, element e1(i) simultaneously forming a dielectric film containing a Si—N bond on the upper surface and a bottom surface and sidewalls of the trench, 173–306
- Claim 9, element e2wherein a top/bottom portion of the dielectric film formed on the upper surface and the bottom surface and a sidewall portion of the dielectric film formed on the sidewalls are given different chemical resistance properties by bombardment of a plasma excited by applying voltage in a reaction space between two electrodes between which the substrate is placed in parallel to the two electrodes; 308–701
- Claim 9, element e3(ii) substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the dielectric film by etching which removes the one of the top/bottom portion and the sidewall portion of the dielectric film more predominantly than the other according to the different chemical resistance properties; and 708–1030
- Claim 9, element e4(iii) obtaining a reference plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, 1042–1248
- Claim 9, element e5wherein the plasma in step (i) is a capacitively coupled plasma (CCP) which is excited by applying RF power to one of the two electrodes, 1250–1386
- Claim 9, element e6wherein plasma density is higher than the reference plasma density, 1388–1454
- Claim 9, element e7wherein the etching in step (ii) removes the top/bottom portion of the dielectric film selectively relative to the sidewall portion of the dielectric film, 1456–1610
- Claim 9, element e8wherein obtaining the reference plasma density comprises performing the forming of dielectric films as recited in step (i), then determining the chemical resistance property by etching as recited in step (ii), then repeating these steps for a plurality of times using different plasma density values, then obtaining the reference ion plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, 1612–2130
- Claim 9, element e9wherein the plasma density is modulated by tuning a ratio of high frequency RF power to low frequency RF power constituting the RF power, 2132–2268
- Claim 9, element e10wherein the plasma density increases by decreasing the ratio, 2270–2330
- Claim 9, element e11wherein the high-frequency RF power has a frequency of 1 MHz or higher and the low-frequency RF power has a frequency of less than 1 MHz.2332–2468
3 dependent claims: 10 to 12 (10, 11 on claim 9; 12 on 11)
Claim 10
Depends on claim 9.
10. The method according to claim 9 , further comprising,
- Claim 10, element e1prior to steps (i) and (ii), repeating the following steps to determine the reference plasma density: 58–158
- Claim 10, element e2simultaneously forming a dielectric film under the same conditions as in step (i) except that the ratio is changed as a variable; and 160–288
- Claim 10, element e3substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the dielectric film by wet etching under the same conditions as in step (ii).294–474
Claim 11
Depends on claim 9.
11. The method according to claim 9 , wherein
- Claim 11, element e1the ratio of high frequency RF power to low frequency RF power is 0/100 to 95/5.46–125
Claim 12
Depends on claim 11.
12. The method according to claim 11 , wherein
- Claim 12, element e1the RF power consists of the low frequency RF power.47–98
1. A method for fabricating a layer structure constituted by a dielectric film containing a Si—N bond in a trench formed in an upper surface of a substrate, comprising: (i) simultaneously forming a dielectric film containing a Si—N bond on the upper surface and a bottom surface and sidewalls of the trench, wherein a top/bottom portion of the dielectric film formed on the upper surface and the bottom surface and a sidewall portion of the dielectric film formed on the sidewalls are given different chemical resistance properties by bombardment of a plasma excited by applying voltage in a reaction space between two electrodes between which the substrate is placed in parallel to the two electrodes; (ii) substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the dielectric film by etching which removes the one of the top/bottom portion and the sidewall portion of the dielectric film more predominantly than the other according to the different chemical resistance properties; and (iii) obtaining a reference plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, wherein the plasma in step (i) is a capacitively coupled plasma (CCP) which is excited by applying RF power to one of the two electrodes, wherein plasma density is higher than the reference plasma density, wherein the etching in step (ii) removes the top/bottom portion of the dielectric film selectively relative to the sidewall portion of the dielectric film, wherein obtaining the reference plasma density comprises performing the forming of dielectric films as recited in step (i), then determining the chemical resistance property by etching as recited in step (ii), then repeating these steps for a plurality of times using different plasma density values, then obtaining the reference plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, and wherein the dielectric film is a SiN film.
2. The method according to claim 1 , wherein in step (i), the dielectric film is formed by plasma-enhanced atomic layer deposition (PEALD).
3. The method according to claim 1 , wherein the plasma is a plasma of Ar, N 2 , or O 2 .
4. The method according to claim 1 , wherein in step (i), a halogenated silane is used as a precursor.
5. The method according to claim 1 , wherein the etching is the wet etching, which is conducted using a solution of hydrogen fluoride (HF) or phosphoric acid.
6. A method for fabricating a layer structure constituted by a dielectric film containing a Si—N bond in a trench formed in an upper surface of a substrate, comprising: (i) simultaneously forming a dielectric film containing a Si—N bond on the upper surface and a bottom surface and sidewalls of the trench, wherein a top/bottom portion of the dielectric film formed on the upper surface and the bottom surface and a sidewall portion of the dielectric film formed on the sidewalls are given different chemical resistance properties by bombardment of a plasma excited by applying voltage in a reaction space between two electrodes between which the substrate is placed in parallel to the two electrodes; (ii) substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the dielectric film by etching which removes the one of the top/bottom portion and the sidewall portion of the dielectric film more predominantly than the other according to the different chemical resistance properties; and (iii) obtaining a reference plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, wherein the plasma in step (i) is a capacitively coupled plasma (CCP) which is excited by applying RF power to one of the two electrodes, wherein plasma density is higher than the reference plasma density, wherein the etching in step (ii) removes the top/bottom portion of the dielectric film selectively relative to the sidewall portion of the dielectric film, wherein obtaining the reference plasma density comprises performing the forming of dielectric films as recited in step (i), then determining the chemical resistance property by etching as recited in step (ii), then repeating these steps for a plurality of times using different plasma density values, then obtaining the reference plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, wherein the plasma density is modulated by tuning the pressure in the reaction space, wherein the plasma density increases by lowering the pressure.
7. The method according to claim 6 , further comprising, prior to steps (i) and (ii), repeating the following steps to determine the reference plasma density: simultaneously forming a dielectric film under the same conditions as in step (i) except that the pressure is changed as a variable; and substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the dielectric film by etching under the same conditions as in step (ii).
8. The method according to claim 6 , wherein the pressure in step (i) is controlled below 300 Pa.
9. A method for fabricating a layer structure constituted by a dielectric film containing a Si—N bond in a trench formed in an upper surface of a substrate, comprising: (i) simultaneously forming a dielectric film containing a Si—N bond on the upper surface and a bottom surface and sidewalls of the trench, wherein a top/bottom portion of the dielectric film formed on the upper surface and the bottom surface and a sidewall portion of the dielectric film formed on the sidewalls are given different chemical resistance properties by bombardment of a plasma excited by applying voltage in a reaction space between two electrodes between which the substrate is placed in parallel to the two electrodes; (ii) substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the dielectric film by etching which removes the one of the top/bottom portion and the sidewall portion of the dielectric film more predominantly than the other according to the different chemical resistance properties; and (iii) obtaining a reference plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, wherein the plasma in step (i) is a capacitively coupled plasma (CCP) which is excited by applying RF power to one of the two electrodes, wherein plasma density is higher than the reference plasma density, wherein the etching in step (ii) removes the top/bottom portion of the dielectric film selectively relative to the sidewall portion of the dielectric film, wherein obtaining the reference plasma density comprises performing the forming of dielectric films as recited in step (i), then determining the chemical resistance property by etching as recited in step (ii), then repeating these steps for a plurality of times using different plasma density values, then obtaining the reference ion plasma density at which the chemical resistance properties of the top/bottom portion of the dielectric film and the sidewall portion of the dielectric film are substantially equivalent, wherein the plasma density is modulated by tuning a ratio of high frequency RF power to low frequency RF power constituting the RF power, wherein the plasma density increases by decreasing the ratio, wherein the high-frequency RF power has a frequency of 1 MHz or higher and the low-frequency RF power has a frequency of less than 1 MHz.
10. The method according to claim 9 , further comprising, prior to steps (i) and (ii), repeating the following steps to determine the reference plasma density: simultaneously forming a dielectric film under the same conditions as in step (i) except that the ratio is changed as a variable; and substantially removing either one of but not both of the top/bottom portion and the sidewall portion of the dielectric film by wet etching under the same conditions as in step (ii).
11. The method according to claim 9 , wherein the ratio of high frequency RF power to low frequency RF power is 0/100 to 95/5.
12. The method according to claim 11 , wherein the RF power consists of the low frequency RF power.
13. The method according to claim 1 , wherein no annealing is conducted between steps (i) and (ii).
The text of each claim as printed, for pasting a claim word for word. The links in the tree view name the same claims and elements.
Status
active
As of 2026-11-17, the USPTO record for US 10529554 shows no unresolved maintenance-fee lapse, and the term end computed from the dates in that record is 2036-02-19 (20 years from the filing of a parent application on 2016-02-19), a date not yet passed (data version 20261117.2).
- Basis
- term_20y (20 years from the filing of a parent application on 2016-02-19)
- Term end
- 2036-02-19 Computed from the dates in the USPTO record
- Fee lapse
- none on record
- Reinstatement
- none on record; reinstatement_possible: false, not lapsed
- As of
- 2026-11-17
- Data version
- 20261117.2
A fact about the record with its basis and its as-of date, not legal advice.
Citations
References cited on the grant: 1211 US patent documents · Cited by: 365 US patents in this data · Lists through the API: /api/v1/patent/us_patent_citation/10529554/ (needs a free key, as the links under Get this as data)
Family outside the US
Google Patents Public Datasets lists no publication outside the US in this patent's family (read 2026-10-15).
This patent's family on USPTO Global Dossier
Family data from Google Patents Public Datasets, used under CC BY 4.0.
Record JSON
{
"patent_id": "10529554",
"status": "active",
"basis": [
"term_20y"
],
"reinstatement_possible": false,
"reinstatement_basis": "not lapsed",
"expiry_date_estimated": "2036-02-19",
"lapse_date": null,
"reinstated_date": null,
"as_of": "2026-11-17",
"data_version": "20261117.2",
"catalog_data_version": "20261117.2",
"permalink": "https://patentref.io/p/10529554?v=20261117.2",
"next_steps": [
{
"kind": "record",
"url": "https://patentref.io/p/10529554?v=20261117.2",
"audience": "human"
},
{
"kind": "patent",
"url": "https://patentref.io/api/v1/patent/10529554/",
"audience": "agent"
},
{
"kind": "fee_events",
"tool": "uspto_patent_center",
"url": "https://patentcenter.uspto.gov/applications?patentNumber=10529554",
"audience": "agent"
}
]
}
Get this as data
- Full record
/api/v1/patent/10529554/ - Status record
/api/v1/lapse/status/10529554/ - Claim tree
/api/v1/structure/claims/10529554/ - Brief
/api/v1/structure/brief/10529554/