US 10546741
Selective growth method
Granted 2020-01-28 · Filed 2018-03-20 · Application 15/926,405 · Utility · Kind B2 · Prior publication US 2018/0286667 A1, 2018-10-04
- Assignee as printed
- TOKYO ELECTRON LIMITED, Tokyo (JP) · PatentsView label: Tokyo Electron Limited
- Inventors
- Hiroki Murakami, Nirasaki (JP); Akira Shimizu, Nirasaki (JP)
- CPC, current
- H01L21/02164; H10P14/69215; H01L21/0217; H01L21/02219; H01L21/0228; H01L21/28562; H01L21/76829; H01L21/76849; H01L21/76879; H10P14/432; H10P14/6339; H10P14/6682; H10P14/6687; H10P14/69433; H10W20/037; H10W20/057; H10W20/074; H01L21/02532; H01L21/0262; H01L21/32; H10P14/24; H10P14/3411; H10P14/61
Abstract
A selective growth method of selectively growing a thin film on an underlayer, on which an insulating film and a conductive film are exposed, includes: preparing a workpiece having the underlayer on which the insulating film and the conductive film are exposed; and selectively growing a silicon-based insulating film on the insulating film by repeating a plurality of times a first step of adsorbing an aminosilane-based gas onto the insulating film and the conductive film and a second step of supplying a reaction gas for reacting with the adsorbed aminosilane-based gas to form the silicon-based insulating film, wherein the conductive film is vaporized by reaction with the reaction gas so that the conductive film is reduced in thickness.
The claims as the USPTO long-text file prints them (text data version 20261117.3), split by PatentRef's claim parser (structure version 2): each claim's opening words, then one row for each element with its character offsets in the claim text, and the dependent claims under the claim they refer to. The split describes the text; it is not a reading of it. Each claim and each element has a link of its own. How the links are made.
Claim 1
Independent claim.
1. A selective growth method of selectively growing a thin film on an underlayer on which an insulating film and a conductive film are exposed, comprising:
- Claim 1, element e1preparing a workpiece having the underlayer on which the insulating film and the conductive film are exposed; and 156–264
- Claim 1, element e2selectively growing a silicon-based insulating film on the insulating film by repeating a cycle a plurality of times, the cycle including: 270–407
- Claim 1, element e3a first step of adsorbing an aminosilane-based gas onto the insulating film and the conductive film; and 409–508
- Claim 1, element e4a second step of supplying a reaction gas to the workpiece such that the silicon-based insulating film is formed on the insulating film by the reaction gas acting on the aminosilane-based gas adsorbed onto the insulating film, and the conductive film is vaporized and reduced in thickness by the reaction gas acting on the conductive film.514–852
9 dependent claims: 2 to 10 (2, 3, 5, 8 on claim 1; 4 on 3; 6, 7 on 5; 9, 10 on 8)
Claim 2
Depends on claim 1.
2. The method of claim 1 , further comprising:
- Claim 2, element e1removing the grown silicon-based insulating film or the grown conductive film.47–124
Claim 3
Depends on claim 1.
3. The method of claim 1 , wherein
- Claim 3, element e1the aminosilane-based gas contains two or more hydrocarbon groups existing in one molecule.35–125
Claim 4
Depends on claim 3.
4. The method of claim 3 , wherein
- Claim 4, element e1the aminosilane-based gas contains four or more methyl groups existing in one molecule when the hydrocarbon group is a methyl group.35–166
Claim 5
Depends on claim 1.
5. The method of claim 1 , wherein
- Claim 5, element e1the silicon-based insulating film is a silicon oxide film, the reaction gas is an oxidizing agent, and the conductive film is made of a material which is oxidized by the oxidizing agent and is vaporized.35–237
Claim 6
Depends on claim 5.
6. The method of claim 5 , wherein
- Claim 6, element e1the conductive film is a ruthenium film or a carbon film.35–91
Claim 7
Depends on claim 5.
7. The method of claim 5 , wherein
- Claim 7, element e1the oxidizing agent is selected from an ozone gas, an O 2 gas, an O 2 /H 2 mixed gas, and an H 2 O gas.35–137
Claim 8
Depends on claim 1.
8. The method of claim 1 , wherein
- Claim 8, element e1the silicon-based insulating film is a silicon nitride film, the reaction gas is a nitriding agent, and the conductive film is made of a material which is nitrided by the nitriding agent and is vaporized.35–238
Claim 9
Depends on claim 8.
9. The method of claim 8 , wherein
- Claim 9, element e1the conductive film is a germanium film.35–74
Claim 10
Depends on claim 8.
10. The method of claim 8 , wherein
- Claim 10, element e1the nitriding agent is selected from an ammonia gas, a hydrazine-based gas, and a hydrogen gas.36–130
Claim 11
Independent claim.
11. A selective growth method of selectively growing a thin film on an underlayer on which an insulating film and a conductive film are exposed, comprising:
- Claim 11, element e1preparing a workpiece having the underlayer on which the insulating film and the conductive film are exposed; 157–265
- Claim 11, element e2selectively growing a silicon-based insulating film on the insulating film by repeating a cycle a plurality of times, the cycle including: 267–404
- Claim 11, element e3a first step of adsorbing an aminosilane-based gas onto the insulating film and the conductive film; and 406–505
- Claim 11, element e4a second step of supplying a reaction gas to form to the workpiece such that the silicon-based insulating film is formed on the insulating film by the reaction gas acting on the aminosilane-based gas adsorbed onto the insulating film, and the conductive film is vaporized and reduced in thickness by the reaction gas acting on the conductive film; and 511–857
- Claim 11, element e5subsequently, selectively growing the conductive film, 863–916
- Claim 11, element e6wherein the selectively growing a silicon-based insulating film and the selectively growing the conductive film are performed a predetermined number of times.918–1075
1 dependent claim: 12 (12 on claim 11)
Claim 12
Depends on claim 11.
12. The method of claim 11 , wherein
- Claim 12, element e1the method is ended in either of the selectively growing a silicon-based insulating film and the selectively growing the conductive film.37–173
Claim 13
Independent claim.
13. A selective growth method of selectively growing a thin film on an underlayer on which an insulating film and a first conductive film are exposed, comprising:
- Claim 13, element e1preparing a workpiece having the underlayer on which the insulating film and a metal film as the first conductive film are exposed; 163–293
- Claim 13, element e2selectively growing a second conductive film on the metal film; and 295–357
- Claim 13, element e3selectively growing a silicon-based insulating film on the insulating film by repeating a cycle a plurality of times, the cycle including: 363–500
- Claim 13, element e4a first step of adsorbing an aminosilane-based gas onto the insulating film and the second conductive film; and 502–608
- Claim 13, element e5a second step of supplying a reaction gas to the workpiece such that the silicon-based insulating film is formed on the insulating film by the reaction gas acting on the aminosilane-based gas adsorbed onto the insulating film, and the second conductive film is vaporized and reduced in thickness by reaction with the reaction gas acting on the second conductive film.614–980
1 dependent claim: 14 (14 on claim 13)
Claim 14
Depends on claim 13.
14. The method of claim 13 , wherein
- Claim 14, element e1the metal film is made of a material selected from a group consisting of tungsten (W), vanadium (V), chromium (Cr), manganese (Mn), iron (Fe), cobalt (Co), nickel (Ni), zinc (Zn), gallium (Ga), germanium (Ge), silicon (Si), zirconium (Zr), niobium (Nb), molybdenum (Mo), technetium (Tc), hafnium (Hf), rhodium (Rh), palladium (Pd), indium (In), tin (Sn), tantalum (Ta), rhenium (Re), osmium (Os), iridium (Ir), platinum (Pt), and gold (Au).37–476
Claim 15
Independent claim.
15. A selective growth method of selectively growing a thin film on an underlayer on which an insulating film and a first conductive film are exposed, comprising:
- Claim 15, element e1preparing a workpiece having the underlayer on which the insulating film and a metal film as the first conductive film are exposed; 163–293
- Claim 15, element e2selectively growing a second conductive film on the metal film; 295–357
- Claim 15, element e3selectively growing a silicon-based insulating film on the insulating film by repeating a cycle a plurality of times, the cycle including: 359–496
- Claim 15, element e4a first step of adsorbing an aminosilane-based gas onto the insulating film and the second conductive film; and 498–604
- Claim 15, element e5a second step of supplying a reaction gas to the workpiece such that the silicon-based insulating film is formed on the insulating film by the reaction gas acting on the aminosilane-based gas adsorbed onto the insulating film, and the second conductive film is vaporized and reduced in thickness by the reaction gas acting on the second conductive film; and 610–962
- Claim 15, element e6selectively growing the second conductive film, 968–1014
- Claim 15, element e7wherein the selectively growing a silicon-based insulating film and the selectively growing the second conductive film are performed a predetermined number of times.1016–1180
1. A selective growth method of selectively growing a thin film on an underlayer on which an insulating film and a conductive film are exposed, comprising: preparing a workpiece having the underlayer on which the insulating film and the conductive film are exposed; and selectively growing a silicon-based insulating film on the insulating film by repeating a cycle a plurality of times, the cycle including: a first step of adsorbing an aminosilane-based gas onto the insulating film and the conductive film; and a second step of supplying a reaction gas to the workpiece such that the silicon-based insulating film is formed on the insulating film by the reaction gas acting on the aminosilane-based gas adsorbed onto the insulating film, and the conductive film is vaporized and reduced in thickness by the reaction gas acting on the conductive film.
2. The method of claim 1 , further comprising: removing the grown silicon-based insulating film or the grown conductive film.
3. The method of claim 1 , wherein the aminosilane-based gas contains two or more hydrocarbon groups existing in one molecule.
4. The method of claim 3 , wherein the aminosilane-based gas contains four or more methyl groups existing in one molecule when the hydrocarbon group is a methyl group.
5. The method of claim 1 , wherein the silicon-based insulating film is a silicon oxide film, the reaction gas is an oxidizing agent, and the conductive film is made of a material which is oxidized by the oxidizing agent and is vaporized.
6. The method of claim 5 , wherein the conductive film is a ruthenium film or a carbon film.
7. The method of claim 5 , wherein the oxidizing agent is selected from an ozone gas, an O 2 gas, an O 2 /H 2 mixed gas, and an H 2 O gas.
8. The method of claim 1 , wherein the silicon-based insulating film is a silicon nitride film, the reaction gas is a nitriding agent, and the conductive film is made of a material which is nitrided by the nitriding agent and is vaporized.
9. The method of claim 8 , wherein the conductive film is a germanium film.
10. The method of claim 8 , wherein the nitriding agent is selected from an ammonia gas, a hydrazine-based gas, and a hydrogen gas.
11. A selective growth method of selectively growing a thin film on an underlayer on which an insulating film and a conductive film are exposed, comprising: preparing a workpiece having the underlayer on which the insulating film and the conductive film are exposed; selectively growing a silicon-based insulating film on the insulating film by repeating a cycle a plurality of times, the cycle including: a first step of adsorbing an aminosilane-based gas onto the insulating film and the conductive film; and a second step of supplying a reaction gas to form to the workpiece such that the silicon-based insulating film is formed on the insulating film by the reaction gas acting on the aminosilane-based gas adsorbed onto the insulating film, and the conductive film is vaporized and reduced in thickness by the reaction gas acting on the conductive film; and subsequently, selectively growing the conductive film, wherein the selectively growing a silicon-based insulating film and the selectively growing the conductive film are performed a predetermined number of times.
12. The method of claim 11 , wherein the method is ended in either of the selectively growing a silicon-based insulating film and the selectively growing the conductive film.
13. A selective growth method of selectively growing a thin film on an underlayer on which an insulating film and a first conductive film are exposed, comprising: preparing a workpiece having the underlayer on which the insulating film and a metal film as the first conductive film are exposed; selectively growing a second conductive film on the metal film; and selectively growing a silicon-based insulating film on the insulating film by repeating a cycle a plurality of times, the cycle including: a first step of adsorbing an aminosilane-based gas onto the insulating film and the second conductive film; and a second step of supplying a reaction gas to the workpiece such that the silicon-based insulating film is formed on the insulating film by the reaction gas acting on the aminosilane-based gas adsorbed onto the insulating film, and the second conductive film is vaporized and reduced in thickness by reaction with the reaction gas acting on the second conductive film.
14. The method of claim 13 , wherein the metal film is made of a material selected from a group consisting of tungsten (W), vanadium (V), chromium (Cr), manganese (Mn), iron (Fe), cobalt (Co), nickel (Ni), zinc (Zn), gallium (Ga), germanium (Ge), silicon (Si), zirconium (Zr), niobium (Nb), molybdenum (Mo), technetium (Tc), hafnium (Hf), rhodium (Rh), palladium (Pd), indium (In), tin (Sn), tantalum (Ta), rhenium (Re), osmium (Os), iridium (Ir), platinum (Pt), and gold (Au).
15. A selective growth method of selectively growing a thin film on an underlayer on which an insulating film and a first conductive film are exposed, comprising: preparing a workpiece having the underlayer on which the insulating film and a metal film as the first conductive film are exposed; selectively growing a second conductive film on the metal film; selectively growing a silicon-based insulating film on the insulating film by repeating a cycle a plurality of times, the cycle including: a first step of adsorbing an aminosilane-based gas onto the insulating film and the second conductive film; and a second step of supplying a reaction gas to the workpiece such that the silicon-based insulating film is formed on the insulating film by the reaction gas acting on the aminosilane-based gas adsorbed onto the insulating film, and the second conductive film is vaporized and reduced in thickness by the reaction gas acting on the second conductive film; and selectively growing the second conductive film, wherein the selectively growing a silicon-based insulating film and the selectively growing the second conductive film are performed a predetermined number of times.
The text of each claim as printed, for pasting a claim word for word. The links in the tree view name the same claims and elements.
Status
active
As of 2026-11-17, the USPTO record for US 10546741 shows no unresolved maintenance-fee lapse, and the term end computed from the dates in that record is 2038-03-20 (20 years from filing), a date not yet passed (data version 20261117.2).
- Basis
- term_20y (20 years from filing)
- Term end
- 2038-03-20 Computed from the dates in the USPTO record
- Fee lapse
- none on record
- Reinstatement
- none on record; reinstatement_possible: false, not lapsed
- As of
- 2026-11-17
- Data version
- 20261117.2
A fact about the record with its basis and its as-of date, not legal advice.
Citations
References cited on the grant: 6 US patent documents · Cited by: 48 US patents in this data · Lists through the API: /api/v1/patent/us_patent_citation/10546741/ (needs a free key, as the links under Get this as data)
Family outside the US
Publications outside the US that Google Patents Public Datasets lists in the same patent family as US 10546741 (read 2026-10-15). Their legal status is not shown here.
| Office | Number | Kind | Published |
|---|---|---|---|
| CN | 108695151 | A | 2018-10-23 |
| CN | 108695151 | B | 2023-08-22 |
| JP | 2018170409 | A | 2018-11-01 |
| JP | 6832776 | B2 | 2021-02-24 |
| KR | 20180111537 | A | 2018-10-11 |
| KR | 102264574 | B1 | 2021-06-11 |
| TW | 201901749 | A | 2019-01-01 |
| TW | I716675 | B | 2021-01-21 |
This patent's family on USPTO Global Dossier
Family data from Google Patents Public Datasets, used under CC BY 4.0.
Record JSON
{
"patent_id": "10546741",
"status": "active",
"basis": [
"term_20y"
],
"reinstatement_possible": false,
"reinstatement_basis": "not lapsed",
"expiry_date_estimated": "2038-03-20",
"lapse_date": null,
"reinstated_date": null,
"as_of": "2026-11-17",
"data_version": "20261117.2",
"catalog_data_version": "20261117.2",
"permalink": "https://patentref.io/p/10546741?v=20261117.2",
"next_steps": [
{
"kind": "record",
"url": "https://patentref.io/p/10546741?v=20261117.2",
"audience": "human"
},
{
"kind": "patent",
"url": "https://patentref.io/api/v1/patent/10546741/",
"audience": "agent"
},
{
"kind": "fee_events",
"tool": "uspto_patent_center",
"url": "https://patentcenter.uspto.gov/applications?patentNumber=10546741",
"audience": "agent"
}
]
}
Get this as data
- Full record
/api/v1/patent/10546741/ - Status record
/api/v1/lapse/status/10546741/ - Claim tree
/api/v1/structure/claims/10546741/ - Brief
/api/v1/structure/brief/10546741/
These four links need a free key (1,000 requests a month). Opened in a browser, which sends no key, they answer 403. Get a free key on the sign-up page, then send it in the X-Api-Key header. To see the shape of an answer without a key, open Try it.