US 10840135
Flat metal features for microelectronics applications
Granted 2020-11-17 · Filed 2019-09-06 · Application 16/563,512 · Utility · Kind B2 · Prior publication US 2019/0393086 A1, 2019-12-26
- Assignee as printed
- Invensas Corporation, San Jose, CA (US) · PatentsView label: Invensas LLC
- Inventors
- Cyprian Emeka Uzoh, San Jose, CA (US)
- CPC, current
- H01L21/76879; H10W20/056; H01L21/3212; H01L21/76819; H01L21/7684; H10P52/403; H10W20/033; H10W20/044; H10W20/057; H10W20/058; H10W20/062; H01L24/05; H01L2224/034; H01L2224/0347; H01L2224/03602; H01L2224/03848; H01L2224/039; H01L2224/03901; H01L2224/08121; H01L2224/08123; H01L2224/08145; H01L2224/80194; H01L2224/80357; H01L2224/80895 and 14 more
Abstract
Advanced flat metals for microelectronics are provided. While conventional processes create large damascene features that have a dishing defect that causes failure in bonded devices, example systems and methods described herein create large damascene features that are planar. In an implementation, an annealing process creates large grains or large metallic crystals of copper in large damascene cavities, while a thinner layer of copper over the field of a substrate anneals into smaller grains of copper. The large grains of copper in the damascene cavities resist dishing defects during chemical-mechanical planarization (CMP), resulting in very flat damascene features. In an implementation, layers of resist and layers of a second coating material may be applied in various ways to resist dishing during chemical-mechanical planarization (CMP), resulting in very flat damascene features.
The claims as the USPTO long-text file prints them (text data version 20261117.3), split by PatentRef's claim parser (structure version 2): each claim's opening words, then one row for each element with its character offsets in the claim text, and the dependent claims under the claim they refer to. The split describes the text; it is not a reading of it. Each claim and each element has a link of its own. How the links are made.
Claim 1
Independent claim.
1. A method, comprising:
- Claim 1, element e1providing a substrate with at least one cavity at a surface; 25–84
- Claim 1, element e2coating the substrate with a barrier layer and a seed layer in the at least one cavity and on a field of the substrate; 86–204
- Claim 1, element e3applying a mask on the field of the substrate, 206–251
- Claim 1, element e4wherein the mask is applied to the seed layer on the field; 253–311
- Claim 1, element e5filling the at least one cavity with a conductive layer to a level of a top of the seed layer on the field; 313–419
- Claim 1, element e6removing the mask from the field; 421–453
- Claim 1, element e7depositing a metal onto the conductive layer in the at least one cavity and onto the seed layer on the field of the substrate, 455–580
- Claim 1, element e8wherein the conductive layer and metal over the at least one cavity is thicker than the metal over the field; 582–690
- Claim 1, element e9thermally annealing the substrate to generate larger grain metal crystals in the at least one cavity and smaller grain metal crystals in the metal over the field of the substrate; 692–870
- Claim 1, element e10applying an intermediate chemical mechanical polishing (CMP) process on the conductive layer in the at least one cavity and on the metal on the field of the substrate; 872–1038
- Claim 1, element e11planarizing the conductive layer in the at least one cavity down to a level of the barrier layer covering the field of the substrate; and 1040–1172
- Claim 1, element e12removing the barrier layer from the field of the substrate to provide a flat conductive feature in the at least one cavity with a dishing defect of less than 3 nanometers per 10 microns width of the flat conductive feature.1178–1400
9 dependent claims: 2 to 10 (2, 3, 4, 5, 6, 7, 8, 9, 10 on claim 1)
Claim 2
Depends on claim 1.
2. The method of claim 1 , wherein
- Claim 2, element e1a width dimension of the flat conductive feature is more than 25 microns and the dishing defect of the flat conductive feature is less than 10 nm.35–180
Claim 3
Depends on claim 1.
3. The method of claim 1 , wherein
- Claim 3, element e1a width dimension of the flat conductive feature is between 26-150 microns and the dishing defect of the flat conductive feature is less than 20 nm.35–182
Claim 4
Depends on claim 1.
4. The method of claim 1 , wherein
- Claim 4, element e1a grain size of the grain metal crystals in the conductive layer in the at least one cavity is more than 2 times the grain size of the grain metal crystals in the metal on the field.35–216
Claim 5
Depends on claim 1.
5. The method of claim 1 , wherein
- Claim 5, element e1a grain size of the grain metal crystals in the conductive layer in the cavity is more than 5 times the grain size of the grain metal crystals in the metal on the field.35–203
Claim 6
Depends on claim 1.
6. The method of claim 1 , wherein
- Claim 6, element e1a thickness of the conductive layer in the cavity is more than 2 times a thickness of the metal on the field.35–143
Claim 7
Depends on claim 1.
7. The method of claim 1 , wherein
- Claim 7, element e1a thickness of the conductive layer in the cavity is more than 5 times a thickness of the metal on the field.35–143
Claim 8
Depends on claim 1.
8. The method of claim 1 , wherein
- Claim 8, element e1the conductive layer in the cavity comprises a metal alloy.35–93
Claim 9
Depends on claim 1.
9. The method of claim 1 , wherein
- Claim 9, element e1the conductive layer comprises one of copper, nickel, silver, gold, platinum, tungsten, or aluminum or one of their respective alloys.35–168
Claim 10
Depends on claim 1.
10. The method of claim 1 , wherein
- Claim 10, element e1the thermally annealing is performed at a temperature between 25-200° C.36–107
Claim 11
Independent claim.
11. A method, comprising:
- Claim 11, element e1coating a substrate with a barrier layer and a first metallic seed layer in cavities of the substrate and on a field of the substrate; 26–159
- Claim 11, element e2applying a mask to the field of the substrate; 161–206
- Claim 11, element e3applying a second metallic seed layer in the cavities including vertical edges of the mask extending vertical sides of the cavities; 208–339
- Claim 11, element e4depositing a metal to overfill the cavities to a level higher than a top surface of the first metallic seed layer on the field; 341–467
- Claim 11, element e5removing the mask from the field; 469–501
- Claim 11, element e6thermally annealing the substrate, the barrier layer, the first metallic seed layer, the second metallic seed layer, and the metal to make small crystals of grained metal in the first metallic seed layer over the field and large crystals of grained metal in the cavities; 503–773
- Claim 11, element e7applying an intermediate chemical-mechanical planarization (CMP) process on the metal in the cavities and on the first metallic seed layer on the field; 775–926
- Claim 11, element e8planarizing the metal overfilling the cavities down to a level of the barrier layer on the field; and 928–1024
- Claim 11, element e9removing the barrier layer from the field to provide wide metal features with a high degree of flatness in the cavities.1030–1149
7 dependent claims: 12 to 18 (12, 13, 15, 16, 17, 18 on claim 11; 14 on 13)
Claim 12
Depends on claim 11.
12. The method of claim 11 , wherein
- Claim 12, element e1the second metallic seed layer has a thickness of at least 50 nanometers.37–109
Claim 13
Depends on claim 11.
13. The method of claim 11 , further comprising
- Claim 13, element e1thermally annealing the substrate, the barrier layer, the first metallic seed layer, the second metallic seed layer, and the metal while the mask is on the field.48–209
Claim 14
Depends on claim 13.
14. The method of claim 13 , further comprising
- Claim 14, element e1removing the mask with the intermediate chemical-mechanical planarization (CMP) process.48–135
Claim 15
Depends on claim 11.
15. The method of claim 11 , wherein
- Claim 15, element e1a width dimension of one of the wide metal features is greater than 25 microns and a dishing of the wide metal features is less than 10 nm.37–175
Claim 16
Depends on claim 11.
16. The method of claim 11 , wherein
- Claim 16, element e1a width dimension of one of the wide metal features is between 26-150 microns and a dishing of the wide metal features is less than 20 nm.37–174
Claim 17
Depends on claim 11.
17. The method of claim 11 , wherein
- Claim 17, element e1the thermally annealing is performed at a temperature between 85-200° C.37–108
Claim 18
Depends on claim 11.
18. The method of claim 11 , wherein
- Claim 18, element e1the method is carried out at a low temperature and the thermally annealing is performed at an ambient room temperature or a temperature around 25° C.37–185
1. A method, comprising: providing a substrate with at least one cavity at a surface; coating the substrate with a barrier layer and a seed layer in the at least one cavity and on a field of the substrate; applying a mask on the field of the substrate, wherein the mask is applied to the seed layer on the field; filling the at least one cavity with a conductive layer to a level of a top of the seed layer on the field; removing the mask from the field; depositing a metal onto the conductive layer in the at least one cavity and onto the seed layer on the field of the substrate, wherein the conductive layer and metal over the at least one cavity is thicker than the metal over the field; thermally annealing the substrate to generate larger grain metal crystals in the at least one cavity and smaller grain metal crystals in the metal over the field of the substrate; applying an intermediate chemical mechanical polishing (CMP) process on the conductive layer in the at least one cavity and on the metal on the field of the substrate; planarizing the conductive layer in the at least one cavity down to a level of the barrier layer covering the field of the substrate; and removing the barrier layer from the field of the substrate to provide a flat conductive feature in the at least one cavity with a dishing defect of less than 3 nanometers per 10 microns width of the flat conductive feature.
2. The method of claim 1 , wherein a width dimension of the flat conductive feature is more than 25 microns and the dishing defect of the flat conductive feature is less than 10 nm.
3. The method of claim 1 , wherein a width dimension of the flat conductive feature is between 26-150 microns and the dishing defect of the flat conductive feature is less than 20 nm.
4. The method of claim 1 , wherein a grain size of the grain metal crystals in the conductive layer in the at least one cavity is more than 2 times the grain size of the grain metal crystals in the metal on the field.
5. The method of claim 1 , wherein a grain size of the grain metal crystals in the conductive layer in the cavity is more than 5 times the grain size of the grain metal crystals in the metal on the field.
6. The method of claim 1 , wherein a thickness of the conductive layer in the cavity is more than 2 times a thickness of the metal on the field.
7. The method of claim 1 , wherein a thickness of the conductive layer in the cavity is more than 5 times a thickness of the metal on the field.
8. The method of claim 1 , wherein the conductive layer in the cavity comprises a metal alloy.
9. The method of claim 1 , wherein the conductive layer comprises one of copper, nickel, silver, gold, platinum, tungsten, or aluminum or one of their respective alloys.
10. The method of claim 1 , wherein the thermally annealing is performed at a temperature between 25-200° C.
11. A method, comprising: coating a substrate with a barrier layer and a first metallic seed layer in cavities of the substrate and on a field of the substrate; applying a mask to the field of the substrate; applying a second metallic seed layer in the cavities including vertical edges of the mask extending vertical sides of the cavities; depositing a metal to overfill the cavities to a level higher than a top surface of the first metallic seed layer on the field; removing the mask from the field; thermally annealing the substrate, the barrier layer, the first metallic seed layer, the second metallic seed layer, and the metal to make small crystals of grained metal in the first metallic seed layer over the field and large crystals of grained metal in the cavities; applying an intermediate chemical-mechanical planarization (CMP) process on the metal in the cavities and on the first metallic seed layer on the field; planarizing the metal overfilling the cavities down to a level of the barrier layer on the field; and removing the barrier layer from the field to provide wide metal features with a high degree of flatness in the cavities.
12. The method of claim 11 , wherein the second metallic seed layer has a thickness of at least 50 nanometers.
13. The method of claim 11 , further comprising thermally annealing the substrate, the barrier layer, the first metallic seed layer, the second metallic seed layer, and the metal while the mask is on the field.
14. The method of claim 13 , further comprising removing the mask with the intermediate chemical-mechanical planarization (CMP) process.
15. The method of claim 11 , wherein a width dimension of one of the wide metal features is greater than 25 microns and a dishing of the wide metal features is less than 10 nm.
16. The method of claim 11 , wherein a width dimension of one of the wide metal features is between 26-150 microns and a dishing of the wide metal features is less than 20 nm.
17. The method of claim 11 , wherein the thermally annealing is performed at a temperature between 85-200° C.
18. The method of claim 11 , wherein the method is carried out at a low temperature and the thermally annealing is performed at an ambient room temperature or a temperature around 25° C.
The text of each claim as printed, for pasting a claim word for word. The links in the tree view name the same claims and elements.
Status
active
As of 2026-11-17, the USPTO record for US 10840135 shows no unresolved maintenance-fee lapse, and the term end computed from the dates in that record, leaving out a terminal disclaimer it shows without a date, is 2038-05-31 (20 years from the filing of a parent application on 2018-05-31), a date not yet passed; that disclaimer can only make the term end earlier (data version 20261117.2).
- Basis
- term_20y · terminal_disclaimer (20 years from the filing of a parent application on 2018-05-31, a terminal disclaimer on record without a date, which can only make the term end earlier than the date computed from the other dates)
- Term end
- 2038-05-31 Computed from the dates in the USPTO recordThis date leaves out a terminal disclaimer on record that has no date; that disclaimer can only make the term end earlier.
- Fee lapse
- none on record
- Reinstatement
- none on record; reinstatement_possible: false, not lapsed
- As of
- 2026-11-17
- Data version
- 20261117.2
A fact about the record with its basis and its as-of date, not legal advice.
Citations
References cited on the grant: 4 US patent documents · Cited by: 129 US patents in this data · Lists through the API: /api/v1/patent/us_patent_citation/10840135/ (needs a free key, as the links under Get this as data)
Family outside the US
Publications outside the US that Google Patents Public Datasets lists in the same patent family as US 10840135 (read 2026-10-15). Their legal status is not shown here.
| Office | Number | Kind | Published |
|---|---|---|---|
| WO | 2018226618 | A1 | 2018-12-13 |
This patent's family on USPTO Global Dossier
Family data from Google Patents Public Datasets, used under CC BY 4.0.
Record JSON
{
"patent_id": "10840135",
"status": "active",
"basis": [
"term_20y",
"terminal_disclaimer"
],
"reinstatement_possible": false,
"reinstatement_basis": "not lapsed",
"expiry_date_estimated": "2038-05-31",
"lapse_date": null,
"reinstated_date": null,
"as_of": "2026-11-17",
"data_version": "20261117.2",
"catalog_data_version": "20261117.2",
"permalink": "https://patentref.io/p/10840135?v=20261117.2",
"next_steps": [
{
"kind": "record",
"url": "https://patentref.io/p/10840135?v=20261117.2",
"audience": "human"
},
{
"kind": "patent",
"url": "https://patentref.io/api/v1/patent/10840135/",
"audience": "agent"
},
{
"kind": "fee_events",
"tool": "uspto_patent_center",
"url": "https://patentcenter.uspto.gov/applications?patentNumber=10840135",
"audience": "agent"
}
]
}
Get this as data
- Full record
/api/v1/patent/10840135/ - Status record
/api/v1/lapse/status/10840135/ - Claim tree
/api/v1/structure/claims/10840135/ - Brief
/api/v1/structure/brief/10840135/
These four links need a free key (1,000 requests a month). Opened in a browser, which sends no key, they answer 403. Get a free key on the sign-up page, then send it in the X-Api-Key header. To see the shape of an answer without a key, open Try it.