US 10947626
Fluoride corrosion inhibition of metal surfaces
Granted 2021-03-16 · Filed 2016-09-01 · Application 16/321,808 · Utility · Kind B2 · Prior publication US 2020/0354839 A1, 2020-11-12
- Assignee as printed
- Halliburton Energy Services, Inc., Houston, TX (US)
- Inventors
- Tiffany Anne Pinder, Houston, TX (US); Enrique Antonio Reyes, Tomball, TX (US)
- CPC, current
- C23F11/143; C09K8/54; C09K8/74; C23F11/04; E21B41/02; C09K2208/32
Abstract
Certain metal surfaces are often unable to be effectively contacted with fluids containing hydrofluoric acid due to significant corrosion issues. Titanium and titanium alloy surfaces represent but one example. Corrosion inhibitor compositions comprising boron-hydroxyalkyl(amine) compound(s) can be used to suppress such metal corrosion, including that taking place on titanium and titanium alloy surfaces, particularly those in a wellbore or in fluid communication with a wellbore.
The claims as the USPTO long-text file prints them (text data version 20261117.3), split by PatentRef's claim parser (structure version 2): each claim's opening words, then one row for each element with its character offsets in the claim text, and the dependent claims under the claim they refer to. The split describes the text; it is not a reading of it. Each claim and each element has a link of its own. How the links are made.
Claim 1
Independent claim.
1. A method comprising:
- Claim 1, element e1providing a treatment fluid comprising: 24–62
- Claim 1, element e2a fluoride source and a corrosion inhibitor composition comprising an aqueous-based fluid, a boron-hydroxyalkyl(amine) compound, and a methan hydrate inhibitor; 64–223
- Claim 1, element e3introducing the treatment fluid into a downhole location including a metal surface comprising titanium or a titanium alloy, 225–347
- Claim 1, element e4wherein the downhole location is selected from the group consisting of a location in a wellbore penetrating a subterranean formation, a location in fluid communication with the wellbore, and any combination thereof; and 349–563
- Claim 1, element e5suppressing corrosion of the metal surface by the fluoride source with the corrosion inhibitor composition.569–675
6 dependent claims: 2 to 7 (2, 3, 4, 5, 6, 7 on claim 1)
Claim 2
Depends on claim 1.
2. The method of claim 1 , wherein
- Claim 2, element e1the fluoride source is selected from the group consisting of a fluoride ion, hydrofluoric acid, a hydrofluoric acid-generating compound, and any combination thereof.35–199
Claim 3
Depends on claim 1.
3. The method of claim 1 , wherein
- Claim 3, element e1the boron-hydroxyalkyl(amine) compound has a boron-nitrogen molar equivalency of about 1:1.35–125
Claim 4
Depends on claim 1.
4. The method of claim 1 , wherein
- Claim 4, element e1the boron-hydroxyalkyl(amine) compound is selected from the group consisting of triethanolamine borate, a derivative of triethanolamine borate, and any combination thereof, or wherein the boron-hydroxyalkyl(amine) compound is a mixture of a boron source and tri(alkyl alcohol)amine and the alkyl is an ethyl, a propyl, a butyl, a pentyl, or any isomer thereof.35–394
Claim 5
Depends on claim 1.
5. The method of claim 1 , wherein
- Claim 5, element e1the metal surface is located in a subsea drilling and production system.35–106
Claim 6
Depends on claim 1.
6. The method of claim 1 , wherein
- Claim 6, element e1the metal surface is located in a subsea drilling and production system and is selected from the group consisting of a drilling riser, a top stress joint, a bottom stress joint, a downhole casing, and any combination thereof.35–259
Claim 7
Depends on claim 1.
7. The method of claim 1 , wherein
- Claim 7, element e1the metal surface is downhole casing in a geothermal well.35–92
Claim 8
Independent claim.
8. A method comprising:
- Claim 8, element e1introducing a treatment fluid into a downhole location through an umbilical, the treatment fluid comprising: 24–131
- Claim 8, element e2a fluoride source; and 133–150
- Claim 8, element e3a corrosion inhibitor composition comprising an aqueous-based fluid, a boron-hydroxyalkyl(amine) compound, and a methane hydrate inhibitor, 156–294
- Claim 8, element e4wherein the into a downhole location is a subsea drilling and production system which includes a metal surface comprising titanium or a titanium alloy; and 296–446
- Claim 8, element e5suppressing corrosion of the metal surface by the fluoride source with the corrosion inhibitor composition.452–558
8 dependent claims: 9 to 16 (9, 10, 12, 13, 14, 15, 16 on claim 8; 11 on 10)
Claim 9
Depends on claim 8.
9. The method of claim 8 , wherein
- Claim 9, element e1the fluoride source is selected from the group consisting of a fluoride ion, hydrofluoric acid, a hydrofluoric acid-generating compound, and any combination thereof.35–199
Claim 10
Depends on claim 8.
10. The method of claim 8 , further comprising
- Claim 10, element e1preparing the corrosion inhibitor by mixing a boron source and a hydroxyalkyl(amine) prior to the step of introducing a treatment fluid into a downhole location through an umbilical.47–228
Claim 11
Depends on claim 10.
11. The method of claim 10 , wherein
- Claim 11, element e1the hydroxyalkyl(amine) is tri(alkyl alcohol)amine wherein the alkyl is an ethyl, a propyl, a butyl, a pentyl, or any isomer thereof.37–169
Claim 12
Depends on claim 8.
12. The method of claim 8 , wherein
- Claim 12, element e1the corrosion inhibitor is prepared on-the-fly.36–82
Claim 13
Depends on claim 8.
13. The method of claim 8 , wherein
- Claim 13, element e1the boron-hydroxyalkyl(amine) compound is selected from the group consisting of triethanolamine borate, a derivative of triethanolamine borate, and any combination thereof, or wherein the boron-hydroxyalkyl(amine) compound is a mixture of a boron source and tri(alkyl alcohol)amine and the alkyl is an ethyl, a propyl, a butyl, a pentyl, or any isomer thereof.36–395
Claim 14
Depends on claim 8.
14. The method of claim 8 wherein
- Claim 14, element e1the titanium or titanium alloy comprises at least of one Ti Grade 29 alloy, Ti Grade 7 alloy, or CP-Ti.34–136
Claim 15
Depends on claim 8.
15. The method of claim 8 , wherein
- Claim 15, element e1the metal surface is located in a subsea drilling and production system and is selected from the group consisting of a drilling riser, a top stress joint, a bottom stress joint, a downhole casing, and any combination thereof.36–260
Claim 16
Depends on claim 8.
16. The method of claim 8 , wherein
- Claim 16, element e1the metal surface is downhole casing in a geothermal well having a bottomhole temperature greater than about 176° C.36–151
Claim 17
Independent claim.
17. A method comprising:
- Claim 17, element e1providing a treatment fluid comprising: 25–63
- Claim 17, element e2a fluoride source and a corrosion inhibitor composition comprising an aqueous-based fluid and a boron-hydroxyalkyl(amine) compound, 65–195
- Claim 17, element e3wherein the boron-hydroxyalkyl(amine) compound is a reaction product of an amine and a boric acid triester, the boric acid triester selected from the group consisting of 2-ethoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, 2-isopropoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, 2-isopropoxy-4,4,6-trimethyl-1,3,2-dioxaborinane, 2-methoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, tributyl borate, tridecyl borate, triethyl borate, trihexyl borate, triisopropyl borate, 2,4,6-trimethoxyboroxin, trimethyl borate, trioctadecyl borate, tri-n-octyl borate, triphenyl borate, tripropyl borate, tris(4-chlorophenyl) borate, tris(2-cyanoethyl) borate, tris(hexafluoroisopropyl) borate, tris(2,2,2-trifluoroethyl) borate, tris(trimethylsilyl) borate, tritetradecyl borate, tri-o-tolyl borate, and any combination thereof; 197–1004
- Claim 17, element e4introducing the treatment fluid into a downhole location including a metal surface comprising titanium or a titanium alloy, 1006–1128
- Claim 17, element e5wherein the downhole location is selected from the group consisting of a location in a wellbore penetrating a subterranean formation, a location in fluid communication with the wellbore, and any combination thereof; and 1130–1344
- Claim 17, element e6suppressing corrosion of the metal surface by the fluoride source with the corrosion inhibitor composition.1350–1456
Claim 18
Independent claim.
18. A method comprising:
- Claim 18, element e1introducing a treatment fluid into a downhole location through an umbilical, the treatment fluid comprising: 25–132
- Claim 18, element e2a fluoride source; and 134–151
- Claim 18, element e3a corrosion inhibitor composition comprising an aqueous-based fluid and a boron-hydroxyalkyl(amine) compound wherein the boron-hydroxyalkyl(amine) compound is a reaction product of an amine and a boric acid triester, the boric acid triester selected from the group consisting of 2-ethoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, 2-isopropoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, 2-isopropoxy-4,4,6-trimethyl-1,3,2-dioxaborinane, 2-methoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, tributyl borate, tridecyl borate, triethyl borate, trihexyl borate, triisopropyl borate, 2,4,6-trimethoxyboroxin, trimethyl borate, trioctadecyl borate, tri-n-octyl borate, triphenyl borate, tripropyl borate, tris(4-chlorophenyl) borate, tris(2-cyanoethyl) borate, tris(hexafluoroisopropyl) borate, tris(2,2,2-trifluoroethyl) borate, tris(trimethylsilyl) borate, tritetradecyl borate, tri-o-tolyl borate, and any combination thereof, 157–1073
- Claim 18, element e4wherein the into a downhole location is a subsea drilling and production system which includes a metal surface comprising titanium or a titanium alloy; and 1075–1225
- Claim 18, element e5suppressing corrosion of the metal surface by the fluoride source with the corrosion inhibitor composition.1231–1337
1. A method comprising: providing a treatment fluid comprising: a fluoride source and a corrosion inhibitor composition comprising an aqueous-based fluid, a boron-hydroxyalkyl(amine) compound, and a methan hydrate inhibitor; introducing the treatment fluid into a downhole location including a metal surface comprising titanium or a titanium alloy, wherein the downhole location is selected from the group consisting of a location in a wellbore penetrating a subterranean formation, a location in fluid communication with the wellbore, and any combination thereof; and suppressing corrosion of the metal surface by the fluoride source with the corrosion inhibitor composition.
2. The method of claim 1 , wherein the fluoride source is selected from the group consisting of a fluoride ion, hydrofluoric acid, a hydrofluoric acid-generating compound, and any combination thereof.
3. The method of claim 1 , wherein the boron-hydroxyalkyl(amine) compound has a boron-nitrogen molar equivalency of about 1:1.
4. The method of claim 1 , wherein the boron-hydroxyalkyl(amine) compound is selected from the group consisting of triethanolamine borate, a derivative of triethanolamine borate, and any combination thereof, or wherein the boron-hydroxyalkyl(amine) compound is a mixture of a boron source and tri(alkyl alcohol)amine and the alkyl is an ethyl, a propyl, a butyl, a pentyl, or any isomer thereof.
5. The method of claim 1 , wherein the metal surface is located in a subsea drilling and production system.
6. The method of claim 1 , wherein the metal surface is located in a subsea drilling and production system and is selected from the group consisting of a drilling riser, a top stress joint, a bottom stress joint, a downhole casing, and any combination thereof.
7. The method of claim 1 , wherein the metal surface is downhole casing in a geothermal well.
8. A method comprising: introducing a treatment fluid into a downhole location through an umbilical, the treatment fluid comprising: a fluoride source; and a corrosion inhibitor composition comprising an aqueous-based fluid, a boron-hydroxyalkyl(amine) compound, and a methane hydrate inhibitor, wherein the into a downhole location is a subsea drilling and production system which includes a metal surface comprising titanium or a titanium alloy; and suppressing corrosion of the metal surface by the fluoride source with the corrosion inhibitor composition.
9. The method of claim 8 , wherein the fluoride source is selected from the group consisting of a fluoride ion, hydrofluoric acid, a hydrofluoric acid-generating compound, and any combination thereof.
10. The method of claim 8 , further comprising preparing the corrosion inhibitor by mixing a boron source and a hydroxyalkyl(amine) prior to the step of introducing a treatment fluid into a downhole location through an umbilical.
11. The method of claim 10 , wherein the hydroxyalkyl(amine) is tri(alkyl alcohol)amine wherein the alkyl is an ethyl, a propyl, a butyl, a pentyl, or any isomer thereof.
12. The method of claim 8 , wherein the corrosion inhibitor is prepared on-the-fly.
13. The method of claim 8 , wherein the boron-hydroxyalkyl(amine) compound is selected from the group consisting of triethanolamine borate, a derivative of triethanolamine borate, and any combination thereof, or wherein the boron-hydroxyalkyl(amine) compound is a mixture of a boron source and tri(alkyl alcohol)amine and the alkyl is an ethyl, a propyl, a butyl, a pentyl, or any isomer thereof.
14. The method of claim 8 wherein the titanium or titanium alloy comprises at least of one Ti Grade 29 alloy, Ti Grade 7 alloy, or CP-Ti.
15. The method of claim 8 , wherein the metal surface is located in a subsea drilling and production system and is selected from the group consisting of a drilling riser, a top stress joint, a bottom stress joint, a downhole casing, and any combination thereof.
16. The method of claim 8 , wherein the metal surface is downhole casing in a geothermal well having a bottomhole temperature greater than about 176° C.
17. A method comprising: providing a treatment fluid comprising: a fluoride source and a corrosion inhibitor composition comprising an aqueous-based fluid and a boron-hydroxyalkyl(amine) compound, wherein the boron-hydroxyalkyl(amine) compound is a reaction product of an amine and a boric acid triester, the boric acid triester selected from the group consisting of 2-ethoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, 2-isopropoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, 2-isopropoxy-4,4,6-trimethyl-1,3,2-dioxaborinane, 2-methoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, tributyl borate, tridecyl borate, triethyl borate, trihexyl borate, triisopropyl borate, 2,4,6-trimethoxyboroxin, trimethyl borate, trioctadecyl borate, tri-n-octyl borate, triphenyl borate, tripropyl borate, tris(4-chlorophenyl) borate, tris(2-cyanoethyl) borate, tris(hexafluoroisopropyl) borate, tris(2,2,2-trifluoroethyl) borate, tris(trimethylsilyl) borate, tritetradecyl borate, tri-o-tolyl borate, and any combination thereof; introducing the treatment fluid into a downhole location including a metal surface comprising titanium or a titanium alloy, wherein the downhole location is selected from the group consisting of a location in a wellbore penetrating a subterranean formation, a location in fluid communication with the wellbore, and any combination thereof; and suppressing corrosion of the metal surface by the fluoride source with the corrosion inhibitor composition.
18. A method comprising: introducing a treatment fluid into a downhole location through an umbilical, the treatment fluid comprising: a fluoride source; and a corrosion inhibitor composition comprising an aqueous-based fluid and a boron-hydroxyalkyl(amine) compound wherein the boron-hydroxyalkyl(amine) compound is a reaction product of an amine and a boric acid triester, the boric acid triester selected from the group consisting of 2-ethoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, 2-isopropoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, 2-isopropoxy-4,4,6-trimethyl-1,3,2-dioxaborinane, 2-methoxy-4,4,5,5-tetramethyl-1,3,2-dioxaborolane, tributyl borate, tridecyl borate, triethyl borate, trihexyl borate, triisopropyl borate, 2,4,6-trimethoxyboroxin, trimethyl borate, trioctadecyl borate, tri-n-octyl borate, triphenyl borate, tripropyl borate, tris(4-chlorophenyl) borate, tris(2-cyanoethyl) borate, tris(hexafluoroisopropyl) borate, tris(2,2,2-trifluoroethyl) borate, tris(trimethylsilyl) borate, tritetradecyl borate, tri-o-tolyl borate, and any combination thereof, wherein the into a downhole location is a subsea drilling and production system which includes a metal surface comprising titanium or a titanium alloy; and suppressing corrosion of the metal surface by the fluoride source with the corrosion inhibitor composition.
The text of each claim as printed, for pasting a claim word for word. The links in the tree view name the same claims and elements.
Status
expired_fee_nonpayment
As of 2026-11-17, the USPTO maintenance-fee record for US 10947626 has an entry dated 2025-04-21 recording that the patent expired for nonpayment of a maintenance fee, and no reinstatement after it (data version 20261117.2).
- Basis
- fee_lapse:2025-04-21 · term_20y · pta_days:143 (fee-lapse entry dated 2025-04-21, 20 years from filing, plus 143 days of patent term adjustment)
- Term end
- 2037-01-22 Computed from the dates in the USPTO recordThe maintenance-fee entry dated 2025-04-21 records an expiry for nonpayment; the date in this row is computed without the maintenance-fee record.
- Fee lapse
- 2025-04-21
- Reinstatement
- none on record; reinstatement_possible: unknown, 37 CFR 1.378: a petition to accept a delayed maintenance fee on the basis of unintentional delay has no fixed time limit; the fee-event record shows no reinstatement as of 2026-11-17
- As of
- 2026-11-17
- Data version
- 20261117.2
A petition under 37 CFR 1.378 has no fixed time limit; the record does not show whether one would be granted.
A fact about the record with its basis and its as-of date, not legal advice.
Citations
References cited on the grant: 3 US patent documents · Cited by: 52 US patents in this data · Lists through the API: /api/v1/patent/us_patent_citation/10947626/ (needs a free key, as the links under Get this as data)
Family outside the US
Publications outside the US that Google Patents Public Datasets lists in the same patent family as US 10947626 (read 2026-10-15). Their legal status is not shown here.
| Office | Number | Kind | Published |
|---|---|---|---|
| BR | 112019001336 | A2 | 2019-04-30 |
| BR | 112019001336 | B1 | 2021-12-14 |
| WO | 2018044310 | A1 | 2018-03-08 |
This patent's family on USPTO Global Dossier
Family data from Google Patents Public Datasets, used under CC BY 4.0.
Record JSON
{
"patent_id": "10947626",
"status": "expired_fee_nonpayment",
"basis": [
"fee_lapse:2025-04-21",
"term_20y",
"pta_days:143"
],
"reinstatement_possible": "unknown",
"reinstatement_basis": "37 CFR 1.378: a petition to accept a delayed maintenance fee on the basis of unintentional delay has no fixed time limit; the fee-event record shows no reinstatement as of 2026-11-17",
"expiry_date_estimated": "2037-01-22",
"lapse_date": "2025-04-21",
"reinstated_date": null,
"as_of": "2026-11-17",
"data_version": "20261117.2",
"catalog_data_version": "20261117.2",
"permalink": "https://patentref.io/p/10947626?v=20261117.2",
"next_steps": [
{
"kind": "record",
"url": "https://patentref.io/p/10947626?v=20261117.2",
"audience": "human"
},
{
"kind": "patent",
"url": "https://patentref.io/api/v1/patent/10947626/",
"audience": "agent"
},
{
"kind": "fee_events",
"tool": "uspto_patent_center",
"url": "https://patentcenter.uspto.gov/applications?patentNumber=10947626",
"audience": "agent"
}
]
}
Get this as data
- Full record
/api/v1/patent/10947626/ - Status record
/api/v1/lapse/status/10947626/ - Claim tree
/api/v1/structure/claims/10947626/ - Brief
/api/v1/structure/brief/10947626/
These four links need a free key (1,000 requests a month). Opened in a browser, which sends no key, they answer 403. Get a free key on the sign-up page, then send it in the X-Api-Key header. To see the shape of an answer without a key, open Try it.