US 11056348
Bonding surfaces for microelectronics
Granted 2021-07-06 · Filed 2019-04-01 · Application 16/371,402 · Utility · Kind B2 · Prior publication US 2019/0311911 A1, 2019-10-10
- Assignee as printed
- INVENSAS BONDING TECHNOLOGIES, INC., San Jose, CA (US)
- Inventors
- Jeremy Alfred Theil, Mountain View, CA (US)
- CPC, current
- H01L21/31053; H10P95/062; H10P14/69433; H10P50/283; H01L2224/03005; H01L2224/03845; H01L2224/08145; H01L2224/8001; H01L2224/80031; H01L2224/80047; H01L2224/80345; H01L2224/80359; H01L2224/80896; H01L2224/94; H10W72/01353; H10W72/07311; H10W72/07331
Abstract
Improved bonding surfaces for microelectronics are provided. An example method of protecting a dielectric surface for direct bonding during a microelectronics fabrication process includes overfilling cavities and trenches in the dielectric surface with a temporary filler that has an approximately equal chemical and mechanical resistance to a chemical-mechanical planarization (CMP) process as the dielectric bonding surface. The CMP process is applied to the temporary filler to flatten the temporary filler down to the dielectric bonding surface. The temporary filler is then removed with an etchant that is selective to the temporary filler, but nonreactive toward the dielectric surface and toward inner surfaces of the cavities and trenches in the dielectric bonding surface. Edges of the cavities remain sharp, which minimizes oxide artifacts, strengthens the direct bond, and reduces the bonding seam.
The claims as the USPTO long-text file prints them (text data version 20261117.3), split by PatentRef's claim parser (structure version 2): each claim's opening words, then one row for each element with its character offsets in the claim text, and the dependent claims under the claim they refer to. The split describes the text; it is not a reading of it. Each claim and each element has a link of its own. How the links are made.
Claim 1
Independent claim.
1. A method for preparing a surface for direct-bonding during a microelectronics fabrication process, comprising:
- Claim 1, element e1overfilling cavities and trenches in a dielectric surface with a temporary filler, 114–195
- Claim 1, element e2wherein the dielectric surface comprises an oxide layer, 197–252
- Claim 1, element e3wherein the oxide layer comprises a layer of silicon oxide and the temporary filler comprises silicon nitride, and wherein the oxide layer and the temporary filler are indistinguishable to a CMP process such that the CMP process has a 1:1 selectivity to the temporary filler as to the oxide layer with respect to both a chemical component of the CMP process and a mechanical component of the CMP process; 254–657
- Claim 1, element e4applying the CMP process to the temporary filler to planarize the temporary filler down to the dielectric surface; and 659–772
- Claim 1, element e5applying an etchant to the temporary filler to remove the temporary filler from the cavities and trenches, the etchant selective to the temporary filler and nonreactive toward the dielectric surface and toward inner surfaces of the cavities and trenches.778–1031
7 dependent claims: 2 to 8 (2, 3, 4, 8 on claim 1; 5, 6 on 4; 7 on 6)
Claim 2
Depends on claim 1.
2. The method of claim 1 , wherein
- Claim 2, element e1the etchant comprises a phosphoric acid etchant to selectively remove the silicon nitride while being nonreactive with the silicon oxide.35–171
Claim 3
Depends on claim 1.
3. The method of claim 1 , further comprising
- Claim 3, element e1direct-bonding the dielectric surface to another dielectric surface.46–113
Claim 4
Depends on claim 1.
4. The method of claim 1 , further comprising:
- Claim 4, element e1prior to the overfilling, preparing the dielectric surface for direct-bonding during a microelectronics fabrication process.47–170
Claim 5
Depends on claim 4.
5. The method of claim 4 , further comprising
- Claim 5, element e1direct-bonding the dielectric surface to another dielectric surface.46–113
Claim 6
Depends on claim 4.
6. The method of claim 4 , wherein
- Claim 6, element e1preparing the dielectric surface comprises planarizing the dielectric surface to a flatness comprising a depth of field of a photolithography system.35–183
Claim 7
Depends on claim 6.
7. The method of claim 6 , further comprising
- Claim 7, element e1direct-bonding the dielectric surface to another dielectric surface.46–113
Claim 8
Depends on claim 1.
8. The method of claim 1 , further comprising:
- Claim 8, element e1prior to the overfilling, etching the cavities and trenches in the dielectric surface with a first etchant; and 47–153
- Claim 8, element e2stripping resist material from the dielectric surface.159–212
Claim 9
Independent claim.
9. A method, comprising:
- Claim 9, element e1preparing a dielectric surface of a wafer or die for direct-bonding during a microelectronics fabrication process, 25–138
- Claim 9, element e2wherein the dielectric surface comprises an oxide layer; 140–195
- Claim 9, element e3masking the dielectric surface with a resist material for etching a cavity in the dielectric surface; 197–297
- Claim 9, element e4etching the cavity in the dielectric surface with a first etchant; 299–364
- Claim 9, element e5stripping the resist material from the dielectric surface; 366–423
- Claim 9, element e6overflowing the cavity with a temporary filler to preserve edges of the cavity during a chemical-mechanical planarization (CMP) process, 425–560
- Claim 9, element e7wherein the oxide layer comprises a layer of silicon oxide and the temporary filler comprises silicon nitride, and wherein the oxide layer and the temporary filler are indistinguishable to the CMP process such that the CMP process has a 1:1 selectivity to the temporary filler as to the oxide layer with respect to both a chemical component of the CMP process and a mechanical component of the CMP process; 562–967
- Claim 9, element e8applying the CMP process to planarize the temporary filler down to an interface between the temporary filler and the dielectric surface; and 969–1104
- Claim 9, element e9removing the temporary filler from the cavity with a second etchant selective to the temporary filler and nonreactive to the dielectric surface and nonreactive to inner surfaces of the cavity.1110–1301
5 dependent claims: 10 to 14 (10, 11, 12, 14 on claim 9; 13 on 12)
Claim 10
Depends on claim 9.
10. The method of claim 9 , wherein
- Claim 10, element e1the second etchant comprises a phosphoric acid to selectively etch the silicon nitride while remaining nonreactive to the silicon oxide.36–171
Claim 11
Depends on claim 9.
11. The method of claim 9 , wherein
- Claim 11, element e1the cavity has a depth penetrating through a layer of the silicon oxide into an underlying layer below the layer of silicon oxide.36–165
Claim 12
Depends on claim 9.
12. The method of claim 9 , wherein
- Claim 12, element e1preparing the dielectric surface before masking further comprises planarizing the dielectric surface to flatness comprising a depth of field of a photolithography system.36–205
Claim 13
Depends on claim 12.
13. The method of claim 12 , further comprising
- Claim 13, element e1direct-bonding the dielectric surface to another dielectric surface.48–115
Claim 14
Depends on claim 9.
14. The method of claim 9 , further comprising
- Claim 14, element e1direct-bonding the dielectric surface to another dielectric surface.47–114
1. A method for preparing a surface for direct-bonding during a microelectronics fabrication process, comprising: overfilling cavities and trenches in a dielectric surface with a temporary filler, wherein the dielectric surface comprises an oxide layer, wherein the oxide layer comprises a layer of silicon oxide and the temporary filler comprises silicon nitride, and wherein the oxide layer and the temporary filler are indistinguishable to a CMP process such that the CMP process has a 1:1 selectivity to the temporary filler as to the oxide layer with respect to both a chemical component of the CMP process and a mechanical component of the CMP process; applying the CMP process to the temporary filler to planarize the temporary filler down to the dielectric surface; and applying an etchant to the temporary filler to remove the temporary filler from the cavities and trenches, the etchant selective to the temporary filler and nonreactive toward the dielectric surface and toward inner surfaces of the cavities and trenches.
2. The method of claim 1 , wherein the etchant comprises a phosphoric acid etchant to selectively remove the silicon nitride while being nonreactive with the silicon oxide.
3. The method of claim 1 , further comprising direct-bonding the dielectric surface to another dielectric surface.
4. The method of claim 1 , further comprising: prior to the overfilling, preparing the dielectric surface for direct-bonding during a microelectronics fabrication process.
5. The method of claim 4 , further comprising direct-bonding the dielectric surface to another dielectric surface.
6. The method of claim 4 , wherein preparing the dielectric surface comprises planarizing the dielectric surface to a flatness comprising a depth of field of a photolithography system.
7. The method of claim 6 , further comprising direct-bonding the dielectric surface to another dielectric surface.
8. The method of claim 1 , further comprising: prior to the overfilling, etching the cavities and trenches in the dielectric surface with a first etchant; and stripping resist material from the dielectric surface.
9. A method, comprising: preparing a dielectric surface of a wafer or die for direct-bonding during a microelectronics fabrication process, wherein the dielectric surface comprises an oxide layer; masking the dielectric surface with a resist material for etching a cavity in the dielectric surface; etching the cavity in the dielectric surface with a first etchant; stripping the resist material from the dielectric surface; overflowing the cavity with a temporary filler to preserve edges of the cavity during a chemical-mechanical planarization (CMP) process, wherein the oxide layer comprises a layer of silicon oxide and the temporary filler comprises silicon nitride, and wherein the oxide layer and the temporary filler are indistinguishable to the CMP process such that the CMP process has a 1:1 selectivity to the temporary filler as to the oxide layer with respect to both a chemical component of the CMP process and a mechanical component of the CMP process; applying the CMP process to planarize the temporary filler down to an interface between the temporary filler and the dielectric surface; and removing the temporary filler from the cavity with a second etchant selective to the temporary filler and nonreactive to the dielectric surface and nonreactive to inner surfaces of the cavity.
10. The method of claim 9 , wherein the second etchant comprises a phosphoric acid to selectively etch the silicon nitride while remaining nonreactive to the silicon oxide.
11. The method of claim 9 , wherein the cavity has a depth penetrating through a layer of the silicon oxide into an underlying layer below the layer of silicon oxide.
12. The method of claim 9 , wherein preparing the dielectric surface before masking further comprises planarizing the dielectric surface to flatness comprising a depth of field of a photolithography system.
13. The method of claim 12 , further comprising direct-bonding the dielectric surface to another dielectric surface.
14. The method of claim 9 , further comprising direct-bonding the dielectric surface to another dielectric surface.
The text of each claim as printed, for pasting a claim word for word. The links in the tree view name the same claims and elements.
Status
active
As of 2026-11-17, the USPTO record for US 11056348 shows no unresolved maintenance-fee lapse, and the term end computed from the dates in that record is 2039-04-01 (20 years from filing), a date not yet passed (data version 20261117.2).
- Basis
- term_20y (20 years from filing)
- Term end
- 2039-04-01 Computed from the dates in the USPTO record
- Fee lapse
- none on record
- Reinstatement
- none on record; reinstatement_possible: false, not lapsed
- As of
- 2026-11-17
- Data version
- 20261117.2
A fact about the record with its basis and its as-of date, not legal advice.
Citations
References cited on the grant: 59 US patent documents · Cited by: 139 US patents in this data · Lists through the API: /api/v1/patent/us_patent_citation/11056348/ (needs a free key, as the links under Get this as data)
Family outside the US
Google Patents Public Datasets lists no publication outside the US in this patent's family (read 2026-10-15).
This patent's family on USPTO Global Dossier
Family data from Google Patents Public Datasets, used under CC BY 4.0.
Record JSON
{
"patent_id": "11056348",
"status": "active",
"basis": [
"term_20y"
],
"reinstatement_possible": false,
"reinstatement_basis": "not lapsed",
"expiry_date_estimated": "2039-04-01",
"lapse_date": null,
"reinstated_date": null,
"as_of": "2026-11-17",
"data_version": "20261117.2",
"catalog_data_version": "20261117.2",
"permalink": "https://patentref.io/p/11056348?v=20261117.2",
"next_steps": [
{
"kind": "record",
"url": "https://patentref.io/p/11056348?v=20261117.2",
"audience": "human"
},
{
"kind": "patent",
"url": "https://patentref.io/api/v1/patent/11056348/",
"audience": "agent"
},
{
"kind": "fee_events",
"tool": "uspto_patent_center",
"url": "https://patentcenter.uspto.gov/applications?patentNumber=11056348",
"audience": "agent"
}
]
}
Get this as data
- Full record
/api/v1/patent/11056348/ - Status record
/api/v1/lapse/status/11056348/ - Claim tree
/api/v1/structure/claims/11056348/ - Brief
/api/v1/structure/brief/11056348/
These four links need a free key (1,000 requests a month). Opened in a browser, which sends no key, they answer 403. Get a free key on the sign-up page, then send it in the X-Api-Key header. To see the shape of an answer without a key, open Try it.