US 11146238
Film bulk acoustic resonator fabrication method
Granted 2021-10-12 · Filed 2020-08-07 · Application 16/988,189 · Utility · Kind B2 · Prior publication US 2020/0373909 A1, 2020-11-26
- Assignee as printed
- Resonant Inc., Austin, TX (US)
- Inventors
- Robert B. Hammond, Lompoc, CA (US); Patrick Turner, San Bruno, CA (US); Ventsislav Yantchev, Sofia (BG)
- CPC, current
- H03H9/174; H03H9/205; H03H3/02; H03H3/04; H03H9/02015; H03H9/02047; H03H9/02157; H03H9/02228; H03H9/568; H03H2003/023; H03H2003/0442
Abstract
Methods of fabricating acoustic resonators are disclosed. A back surface of a piezoelectric plate is bonded to a surface of a substrate. Thickness measurements are made at a plurality of positions on the piezoelectric plate. Excess material is removed from the front surface of the piezoelectric plate in accordance with the thickness measurements to improve a thickness uniformity of the piezoelectric plate. A conductor pattern is formed on the front surface, the conductor pattern including a plurality of interdigital transducers (IDTs) of a plurality of resonators. Cavities are formed in the substrate such that portions of the single-crystal piezoelectric plate form a plurality of diaphragms spanning respective cavities, wherein interleaved fingers of each IDT of the plurality of IDTs are disposed on a respective one of the plurality of diaphragms.
The claims as the USPTO long-text file prints them (text data version 20261117.3), split by PatentRef's claim parser (structure version 2): each claim's opening words, then one row for each element with its character offsets in the claim text, and the dependent claims under the claim they refer to. The split describes the text; it is not a reading of it. Each claim and each element has a link of its own. How the links are made.
Claim 1
Independent claim.
1. A method of fabricating a plurality of acoustic resonators on a piezoelectric plate having opposed front and back surfaces, the method comprising:
- Claim 1, element e1bonding the back surface of the piezoelectric plate to a surface of a substrate; 150–229
- Claim 1, element e2performing thickness measurements of a thickness of the piezoelectric plate at a plurality of positions on the piezoelectric plate; 231–361
- Claim 1, element e3removing excess material from the front surface of the piezoelectric plate in accordance with the thickness measurements to improve a thickness uniformity of the piezoelectric plate; 363–544
- Claim 1, element e4after removing the excess material, forming a conductor pattern on the front surface of the piezoelectric plate, the conductor pattern including a plurality of interdigital transducers (IDTs) of the plurality of acoustic resonators; and 546–777
- Claim 1, element e5forming cavities in the substrate such that portions of the piezoelectric plate form a plurality of diaphragms spanning respective cavities, 783–922
- Claim 1, element e6wherein, after the cavities and the conductor pattern are formed, interleaved fingers of each IDT of the plurality of IDTs are disposed on a respective one of the plurality of diaphragms.924–1110
9 dependent claims: 2 to 9 and 20 (2, 4, 5, 6, 7, 8, 9, 20 on claim 1; 3 on 2)
Claim 2
Depends on claim 1.
2. The method of claim 1 , wherein
- Claim 2, element e1the front surface of the piezoelectric plate is attached to a sacrificial substrate during the bonding, the method further comprising: 35–168
- Claim 2, element e2removing the sacrificial substrate to expose the front surface of the piezoelectric plate after the bonding.170–277
Claim 3
Depends on claim 2.
3. The method of claim 2 , further comprising:
- Claim 3, element e1polishing the front surface of the piezoelectric plate after removing the sacrificial substrate and before performing thickness measurements.47–187
Claim 4
Depends on claim 1.
4. The method of claim 1 , wherein
- Claim 4, element e1performing thickness measurements further comprises: 35–86
- Claim 4, element e2measuring a respective thickness at each of the plurality of positions using an optical interferometer and/or an optical reflectometer.88–222
Claim 5
Depends on claim 1.
5. The method of claim 1 , wherein
- Claim 5, element e1removing excess material is performed with a scanning ion mill.35–97
Claim 6
Depends on claim 1.
6. The method of claim 1 , wherein
- Claim 6, element e1removing excess material further comprises: 35–77
- Claim 6, element e2removing excess material from the front surface of the piezoelectric plate to make a thickness at any point on the piezoelectric plate essentially equal to a predetermined first thickness.79–266
Claim 7
Depends on claim 1.
7. The method of claim 1 , further comprising:
- Claim 7, element e1after removing the excess material and before forming a conductor pattern, post processing the piezoelectric plate to repair surface damage.47–186
Claim 8
Depends on claim 1.
8. The method of claim 1 , wherein
- Claim 8, element e1the piezoelectric plate and all of the IDTs are configured such that a respective radio frequency signal applied to each IDT excites a respective shear primary acoustic mode within the respective diaphragm.35–240
Claim 9
Depends on claim 1.
9. The method of claim 1 , wherein
- Claim 9, element e1the single-crystal piezoelectric plate is one of lithium niobate and lithium tantalate.35–121
Claim 20
Depends on claim 1.
20. The method of claim 1 , wherein
- Claim 20, element e1removing excess material from the front surface of the piezoelectric plate in accordance with the thickness measurements further comprises: 36–174
- Claim 20, element e2interpolating the thickness measurements to generate a map of the thickness of the piezoelectric plate; and 176–278
- Claim 20, element e3removing excess material from the front surface of the piezoelectric plate in accordance with the map.284–385
Claim 10
Independent claim.
10. A method of fabricating a plurality of acoustic resonators on a piezoelectric plate having opposed front and back surfaces, the method comprising:
- Claim 10, element e1bonding the back surface of the piezoelectric plate to a surface of a substrate; 151–230
- Claim 10, element e2performing thickness measurements of a thickness of the piezoelectric plate at a plurality of positions on the piezoelectric plate; 232–362
- Claim 10, element e3removing excess material from the front surface of the piezoelectric plate in accordance with the thickness measurements to improve a thickness uniformity of the piezoelectric plate; 364–545
- Claim 10, element e4after removing the excess material, selectively thinning portions of the piezoelectric plate from the first thickness to a second thickness less than the first thickness, after selectively thinning portions of the piezoelectric plate, forming a conductor pattern on the front surface of the piezoelectric plate, the conductor pattern including a plurality of interdigital transducers (IDTs) of the plurality of acoustic resonators; and 547–977
- Claim 10, element e5forming cavities in the substrate such that portions of the piezoelectric plate form a plurality of diaphragms spanning respective cavities, 983–1122
- Claim 10, element e6wherein, after the cavities and the conductor pattern are formed: 1124–1188
- Claim 10, element e7interleaved fingers of one or more IDTs of the plurality of IDTs are disposed on respective diaphragms having the first thickness, and interleaved fingers of one or more IDTs of the plurality of IDTs are disposed on respective diaphragms having the second thickness.1190–1455
9 dependent claims: 11 to 19 (11, 13, 14, 15, 16, 17, 18, 19 on claim 10; 12 on 11)
Claim 11
Depends on claim 10.
11. The method of claim 10 , wherein
- Claim 11, element e1the front surface of the piezoelectric plate is attached to a sacrificial substrate during the bonding, the method further comprising: 37–170
- Claim 11, element e2removing the sacrificial substrate to expose the front surface of the piezoelectric plate after the bonding.172–279
Claim 12
Depends on claim 11.
12. The method of claim 11 , further comprising:
- Claim 12, element e1polishing the front surface of the piezoelectric plate after removing the sacrificial substrate and before performing thickness measurements.49–189
Claim 13
Depends on claim 10.
13. The method of claim 10 , wherein
- Claim 13, element e1performing thickness measurements further comprises: 37–88
- Claim 13, element e2measuring a respective thickness at each of the plurality of positions using an optical interferometer and/or an optical reflectometer.90–224
Claim 14
Depends on claim 10.
14. The method of claim 10 , wherein
- Claim 14, element e1removing excess material is performed with a scanning ion mill.37–99
Claim 15
Depends on claim 10.
15. The method of claim 10 , wherein
- Claim 15, element e1removing excess material further comprises: 37–79
- Claim 15, element e2removing excess material from the front surface of the piezoelectric plate to make a thickness at any point on the piezoelectric plate essentially equal to a predetermined first thickness.81–268
Claim 16
Depends on claim 10.
16. The method of claim 10 , further comprising:
- Claim 16, element e1after removing the excess material and before forming a conductor pattern, post processing the piezoelectric plate to repair surface damage.49–188
Claim 17
Depends on claim 10.
17. The method of claim 10 , wherein
- Claim 17, element e1the piezoelectric plate and all of the IDTs are configured such that a respective radio frequency signal applied to each IDT excites a respective shear primary acoustic mode within the respective diaphragm.37–242
Claim 18
Depends on claim 10.
18. The method of claim 10 , wherein
- Claim 18, element e1the single-crystal piezoelectric plate is one of lithium niobate and lithium tantalate.37–123
Claim 19
Depends on claim 10.
19. The method of claim 10 , wherein
- Claim 19, element e1removing excess material from the front surface of the piezoelectric plate in accordance with the thickness measurements further comprises: 37–175
- Claim 19, element e2interpolating the thickness measurements to generate a map of the thickness of the piezoelectric plate; and 177–279
- Claim 19, element e3removing excess material from the front surface of the piezoelectric plate in accordance with the map.285–386
1. A method of fabricating a plurality of acoustic resonators on a piezoelectric plate having opposed front and back surfaces, the method comprising: bonding the back surface of the piezoelectric plate to a surface of a substrate; performing thickness measurements of a thickness of the piezoelectric plate at a plurality of positions on the piezoelectric plate; removing excess material from the front surface of the piezoelectric plate in accordance with the thickness measurements to improve a thickness uniformity of the piezoelectric plate; after removing the excess material, forming a conductor pattern on the front surface of the piezoelectric plate, the conductor pattern including a plurality of interdigital transducers (IDTs) of the plurality of acoustic resonators; and forming cavities in the substrate such that portions of the piezoelectric plate form a plurality of diaphragms spanning respective cavities, wherein, after the cavities and the conductor pattern are formed, interleaved fingers of each IDT of the plurality of IDTs are disposed on a respective one of the plurality of diaphragms.
2. The method of claim 1 , wherein the front surface of the piezoelectric plate is attached to a sacrificial substrate during the bonding, the method further comprising: removing the sacrificial substrate to expose the front surface of the piezoelectric plate after the bonding.
3. The method of claim 2 , further comprising: polishing the front surface of the piezoelectric plate after removing the sacrificial substrate and before performing thickness measurements.
4. The method of claim 1 , wherein performing thickness measurements further comprises: measuring a respective thickness at each of the plurality of positions using an optical interferometer and/or an optical reflectometer.
5. The method of claim 1 , wherein removing excess material is performed with a scanning ion mill.
6. The method of claim 1 , wherein removing excess material further comprises: removing excess material from the front surface of the piezoelectric plate to make a thickness at any point on the piezoelectric plate essentially equal to a predetermined first thickness.
7. The method of claim 1 , further comprising: after removing the excess material and before forming a conductor pattern, post processing the piezoelectric plate to repair surface damage.
8. The method of claim 1 , wherein the piezoelectric plate and all of the IDTs are configured such that a respective radio frequency signal applied to each IDT excites a respective shear primary acoustic mode within the respective diaphragm.
9. The method of claim 1 , wherein the single-crystal piezoelectric plate is one of lithium niobate and lithium tantalate.
10. A method of fabricating a plurality of acoustic resonators on a piezoelectric plate having opposed front and back surfaces, the method comprising: bonding the back surface of the piezoelectric plate to a surface of a substrate; performing thickness measurements of a thickness of the piezoelectric plate at a plurality of positions on the piezoelectric plate; removing excess material from the front surface of the piezoelectric plate in accordance with the thickness measurements to improve a thickness uniformity of the piezoelectric plate; after removing the excess material, selectively thinning portions of the piezoelectric plate from the first thickness to a second thickness less than the first thickness, after selectively thinning portions of the piezoelectric plate, forming a conductor pattern on the front surface of the piezoelectric plate, the conductor pattern including a plurality of interdigital transducers (IDTs) of the plurality of acoustic resonators; and forming cavities in the substrate such that portions of the piezoelectric plate form a plurality of diaphragms spanning respective cavities, wherein, after the cavities and the conductor pattern are formed: interleaved fingers of one or more IDTs of the plurality of IDTs are disposed on respective diaphragms having the first thickness, and interleaved fingers of one or more IDTs of the plurality of IDTs are disposed on respective diaphragms having the second thickness.
11. The method of claim 10 , wherein the front surface of the piezoelectric plate is attached to a sacrificial substrate during the bonding, the method further comprising: removing the sacrificial substrate to expose the front surface of the piezoelectric plate after the bonding.
12. The method of claim 11 , further comprising: polishing the front surface of the piezoelectric plate after removing the sacrificial substrate and before performing thickness measurements.
13. The method of claim 10 , wherein performing thickness measurements further comprises: measuring a respective thickness at each of the plurality of positions using an optical interferometer and/or an optical reflectometer.
14. The method of claim 10 , wherein removing excess material is performed with a scanning ion mill.
15. The method of claim 10 , wherein removing excess material further comprises: removing excess material from the front surface of the piezoelectric plate to make a thickness at any point on the piezoelectric plate essentially equal to a predetermined first thickness.
16. The method of claim 10 , further comprising: after removing the excess material and before forming a conductor pattern, post processing the piezoelectric plate to repair surface damage.
17. The method of claim 10 , wherein the piezoelectric plate and all of the IDTs are configured such that a respective radio frequency signal applied to each IDT excites a respective shear primary acoustic mode within the respective diaphragm.
18. The method of claim 10 , wherein the single-crystal piezoelectric plate is one of lithium niobate and lithium tantalate.
19. The method of claim 10 , wherein removing excess material from the front surface of the piezoelectric plate in accordance with the thickness measurements further comprises: interpolating the thickness measurements to generate a map of the thickness of the piezoelectric plate; and removing excess material from the front surface of the piezoelectric plate in accordance with the map.
20. The method of claim 1 , wherein removing excess material from the front surface of the piezoelectric plate in accordance with the thickness measurements further comprises: interpolating the thickness measurements to generate a map of the thickness of the piezoelectric plate; and removing excess material from the front surface of the piezoelectric plate in accordance with the map.
The text of each claim as printed, for pasting a claim word for word. The links in the tree view name the same claims and elements.
Status
active
As of 2026-11-17, the USPTO record for US 11146238 shows no unresolved maintenance-fee lapse, and the term end computed from the dates in that record is 2038-12-21 (20 years from the filing of a parent application on 2018-12-21), a date not yet passed (data version 20261117.2).
- Basis
- term_20y (20 years from the filing of a parent application on 2018-12-21)
- Term end
- 2038-12-21 Computed from the dates in the USPTO record
- Fee lapse
- none on record
- Reinstatement
- none on record; reinstatement_possible: false, not lapsed
- As of
- 2026-11-17
- Data version
- 20261117.2
A fact about the record with its basis and its as-of date, not legal advice.
Citations
References cited on the grant: 51 US patent documents · Cited by: 58 US patents in this data · Lists through the API: /api/v1/patent/us_patent_citation/11146238/ (needs a free key, as the links under Get this as data)
Family outside the US
Google Patents Public Datasets lists no publication outside the US in this patent's family (read 2026-10-15).
This patent's family on USPTO Global Dossier
Family data from Google Patents Public Datasets, used under CC BY 4.0.
Record JSON
{
"patent_id": "11146238",
"status": "active",
"basis": [
"term_20y"
],
"reinstatement_possible": false,
"reinstatement_basis": "not lapsed",
"expiry_date_estimated": "2038-12-21",
"lapse_date": null,
"reinstated_date": null,
"as_of": "2026-11-17",
"data_version": "20261117.2",
"catalog_data_version": "20261117.2",
"permalink": "https://patentref.io/p/11146238?v=20261117.2",
"next_steps": [
{
"kind": "record",
"url": "https://patentref.io/p/11146238?v=20261117.2",
"audience": "human"
},
{
"kind": "patent",
"url": "https://patentref.io/api/v1/patent/11146238/",
"audience": "agent"
},
{
"kind": "fee_events",
"tool": "uspto_patent_center",
"url": "https://patentcenter.uspto.gov/applications?patentNumber=11146238",
"audience": "agent"
}
]
}
Get this as data
- Full record
/api/v1/patent/11146238/ - Status record
/api/v1/lapse/status/11146238/ - Claim tree
/api/v1/structure/claims/11146238/ - Brief
/api/v1/structure/brief/11146238/
These four links need a free key (1,000 requests a month). Opened in a browser, which sends no key, they answer 403. Get a free key on the sign-up page, then send it in the X-Api-Key header. To see the shape of an answer without a key, open Try it.