US 11148870
Methods of forming repulpable containers
Granted 2021-10-19 · Filed 2020-12-16 · Application 17/123,676 · Utility · Kind B2 · Prior publication US 2021/0101735 A1, 2021-04-08
- Assignee as printed
- Pratt Retail Specialties, LLC, Conyers, GA (US)
- Inventors
- Alan B. Collison, Pierce, NE (US); Reid Borgman, Norfolk, NE (US)
- CPC, current
- B32B5/08; B65D81/3823; B29C70/08; B29C70/12; B29C70/508; B29C70/545; B32B3/04; B32B5/02; B32B5/06; B32B7/09; B32B7/12; B32B7/14; B32B27/32; B32B29/005; B32B29/02; B32B29/08; B65B11/08; B65D5/0227; B65D27/00; B65D27/005; B65D81/3858; D21H13/14; D21H15/10; D21H21/52 and 25 more
Abstract
A method of forming a shipping container includes mixing paper fibers with a binder fiber to form a mixture; disposing the mixture onto a surface to form a layer of the mixture; applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length; and inserting the paper fiber batt within an interior of a corrugated box.
The claims as the USPTO long-text file prints them (text data version 20261117.3), split by PatentRef's claim parser (structure version 2): each claim's opening words, then one row for each element with its character offsets in the claim text, and the dependent claims under the claim they refer to. The split describes the text; it is not a reading of it. Each claim and each element has a link of its own. How the links are made.
Claim 1
Independent claim.
1. A method of forming a shipping container comprising:
- Claim 1, element e1mixing paper fibers with about 0.5% to 25% by weight meltable thermoplastic binder fiber to form a mixture, 56–162
- Claim 1, element e2wherein the thermoplastic binder fiber has a length of between about 0.5 mm to about 16 mm; 164–254
- Claim 1, element e3disposing the mixture onto a surface to form a layer of the mixture; 256–323
- Claim 1, element e4applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length; and 325–420
- Claim 1, element e5coupling the paper fiber batt to a corrugated box, 426–475
- Claim 1, element e6wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%, 477–585
- Claim 1, element e7wherein the repulpability test follows requirements set by Fibre Box Association of Elk Grove Village, Ill., and recited in Voluntary Standard For Repulping and Recycling Corrugated Fiberboard Treated to Improve Its Performance in the Presence of Water and Water Vapor as revised on Aug. 16, 2013.587–883
4 dependent claims: 2 to 5 (2, 4, 5 on claim 1; 3 on 2)
Claim 2
Depends on claim 1.
2. The method according to claim 1 , wherein
- Claim 2, element e1mixing the paper fibers with a binder fiber comprises mixing the paper fibers with a meltable PE/PP bi-component thermoplastic binder fiber.45–184
Claim 3
Depends on claim 2.
3. The method according to claim 2 , wherein
- Claim 3, element e1the thermoplastic binder fibers make up less than 10% by weight of the paper fiber batt.45–132
Claim 4
Depends on claim 1.
4. The method according to claim 1 , wherein
- Claim 4, element e1applying heat to form a paper fiber batt further comprises applying pressure with the heat to form the paper fiber batt.45–164
Claim 5
Depends on claim 1.
5. The method according to claim 1 , wherein
- Claim 5, element e1the step of coupling the paper fiber batt to a corrugated box comprises inserting the paper fiber batt in an interior of the box.45–173
Claim 6
Independent claim.
6. A method of forming a shipping container comprising:
- Claim 6, element e1mixing paper fibers with about 0.5% to 25% by weight meltable PE/PP bi-component binder fiber to form a mixture, 56–167
- Claim 6, element e2wherein the binder fiber has a length of between about 0.5 mm to about 16 mm; 169–245
- Claim 6, element e3disposing the mixture onto a surface to form a layer of the mixture; 247–314
- Claim 6, element e4applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length; and 316–411
- Claim 6, element e5inserting the paper fiber batt within an interior of a corrugated box, 417–486
- Claim 6, element e6wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%, 488–596
- Claim 6, element e7wherein the repulpability test follows requirements set by Fibre Box Association of Elk Grove Village, Ill., and recited in Voluntary Standard For Repulping and Recycling Corrugated Fiberboard Treated to Improve Its Performance in the Presence of Water and Water Vapor as revised on Aug. 16, 2013.598–894
5 dependent claims: 7 to 10 and 23 (7, 8, 9, 23 on claim 6; 10 on 9)
Claim 7
Depends on claim 6.
7. The method according to claim 6 , wherein
- Claim 7, element e1subjecting the binder fibers make up less than 10% by weight of the paper fiber batt.45–129
Claim 8
Depends on claim 6.
8. The method according to claim 6 , wherein
- Claim 8, element e1applying heat to form a paper fiber batt further comprises applying pressure with the heat to form the paper fiber batt.45–164
Claim 9
Depends on claim 6.
9. The method according to claim 6 , further comprising the step of
- Claim 9, element e1encapsulating the paper fiber batt within a paper layer.68–123
Claim 10
Depends on claim 9.
10. The method according to claim 9 , further comprising the step of
- Claim 10, element e1connecting a first paper layer to a second paper layer to form the paper layer encapsulating the paper fiber batt.69–182
Claim 23
Depends on claim 6.
23. The method according to claim 6 , wherein
- Claim 23, element e1the paper fiber batt has a thickness that is at least 1/16 inch.46–109
Claim 11
Independent claim.
11. A method of forming a shipping container comprising:
- Claim 11, element e1mixing paper fibers with about 0.5% to 25% by weight meltable thermoplastic binder fiber to form a mixture; 57–163
- Claim 11, element e2disposing the mixture onto a surface to form a layer of the mixture, the mixture having a density of 1300 to 1600 grams per square meter; 165–301
- Claim 11, element e3applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length; 303–398
- Claim 11, element e4encapsulating the paper fiber batt within a paper layer; and 400–455
- Claim 11, element e5folding the encapsulated paper fiber batt to form a bottom of the shipping container along the fold and also to define lateral edges adjacent to the bottom and a top arranged opposite to the bottom, the top defining an opening, 461–687
- Claim 11, element e6wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%.689–797
4 dependent claims: 12 to 15 (12, 14, 15 on claim 11; 13 on 12)
Claim 12
Depends on claim 11.
12. The method according to claim 11 , further comprising the step of
- Claim 12, element e1sealing at least two lateral edges of the paper layer.70–123
Claim 13
Depends on claim 12.
13. The method according to claim 12 , wherein
- Claim 13, element e1the lateral edges are sealed by heat sealing.47–91
Claim 14
Depends on claim 11.
14. The method according to claim 11 , wherein
- Claim 14, element e1the step of encapsulating the paper fiber batt within the paper layer comprises securing a first paper layer to a second paper layer with the paper fiber batt located between the first paper layer and the second paper layer.47–270
Claim 15
Depends on claim 11.
15. The method according to claim 11 , wherein
- Claim 15, element e1the thermoplastic binder fibers make up less than 10% by weight of the paper fiber batt.47–134
Claim 16
Independent claim.
16. A method of forming a shipping container, the method comprising:
- Claim 16, element e1mixing paper fibers with about 0.5% to 25% by weight meltable PE/PP bi-component binder fiber to form a mixture, the binder fibers being of a length of less than about 24 millimeters; 69–251
- Claim 16, element e2applying heat to form a paper fiber ball from the mixture having a fixed width and fixed length; 253–348
- Claim 16, element e3forming a shipping container from a paper medium, the shipping container defining an interior; 350–443
- Claim 16, element e4securing a paper layer to the paper fiber batt; and 445–491
- Claim 16, element e5surrounding the interior of the shipping container with the paper fiber batt, 497–573
- Claim 16, element e6wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%, 575–683
- Claim 16, element e7wherein the repulpability test follows requirements set by Fibre Box Association of Elk Grove Village, Ill., and recited in Voluntary Standard For Repulping and Recycling Corrugated Fiberboard Treated to Improve Its Performance in the Presence of Water and Water Vapor as revised on Aug. 16, 2013.685–981
6 dependent claims: 17 to 22 (17, 19, 20, 21, 22 on claim 16; 18 on 17)
Claim 17
Depends on claim 16.
17. The method of claim 16 , wherein
- Claim 17, element e1the step of securing the paper layer to the paper fiber batt comprises encapsulating the paper fiber batt within the paper layer.37–165
Claim 18
Depends on claim 17.
18. The method of claim 17 , wherein
- Claim 18, element e1the step of forming the shipping container from the paper medium comprises folding the encapsulated paper fiber batt to form a bottom of the shipping container along the fold and also to define lateral edges adjacent to the bottom and a top arranged opposite to the bottom, the top defining an opening.37–338
Claim 19
Depends on claim 16.
19. The method of claim 16 , wherein
- Claim 19, element e1the thermoplastic binder fiber has a length of between about 0.5 mm to about 16 mm.37–119
Claim 20
Depends on claim 16.
20. The method of claim 16 , wherein
- Claim 20, element e1the step of forming the shipping container from the paper medium comprises forming a corrugated box, and wherein the step of securing the paper layer to the paper fiber batt comprises coupling the paper fiber batt to the corrugated box.37–272
Claim 21
Depends on claim 16.
21. The method of claim 16 , wherein
- Claim 21, element e1the PE/PP bi-component binder fiber makes up less than 10% by weight of the paper fiber batt.37–129
Claim 22
Depends on claim 16.
22. The method of claim 16 , wherein
- Claim 22, element e1about 50% of the PE/PP bi-component binder fiber has a length of about 1 millimeter and about 50% of the PE/PP bi-component binder fiber has a length of about 6 millimeters.37–209
1. A method of forming a shipping container comprising: mixing paper fibers with about 0.5% to 25% by weight meltable thermoplastic binder fiber to form a mixture, wherein the thermoplastic binder fiber has a length of between about 0.5 mm to about 16 mm; disposing the mixture onto a surface to form a layer of the mixture; applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length; and coupling the paper fiber batt to a corrugated box, wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%, wherein the repulpability test follows requirements set by Fibre Box Association of Elk Grove Village, Ill., and recited in Voluntary Standard For Repulping and Recycling Corrugated Fiberboard Treated to Improve Its Performance in the Presence of Water and Water Vapor as revised on Aug. 16, 2013.
2. The method according to claim 1 , wherein mixing the paper fibers with a binder fiber comprises mixing the paper fibers with a meltable PE/PP bi-component thermoplastic binder fiber.
3. The method according to claim 2 , wherein the thermoplastic binder fibers make up less than 10% by weight of the paper fiber batt.
4. The method according to claim 1 , wherein applying heat to form a paper fiber batt further comprises applying pressure with the heat to form the paper fiber batt.
5. The method according to claim 1 , wherein the step of coupling the paper fiber batt to a corrugated box comprises inserting the paper fiber batt in an interior of the box.
6. A method of forming a shipping container comprising: mixing paper fibers with about 0.5% to 25% by weight meltable PE/PP bi-component binder fiber to form a mixture, wherein the binder fiber has a length of between about 0.5 mm to about 16 mm; disposing the mixture onto a surface to form a layer of the mixture; applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length; and inserting the paper fiber batt within an interior of a corrugated box, wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%, wherein the repulpability test follows requirements set by Fibre Box Association of Elk Grove Village, Ill., and recited in Voluntary Standard For Repulping and Recycling Corrugated Fiberboard Treated to Improve Its Performance in the Presence of Water and Water Vapor as revised on Aug. 16, 2013.
7. The method according to claim 6 , wherein subjecting the binder fibers make up less than 10% by weight of the paper fiber batt.
8. The method according to claim 6 , wherein applying heat to form a paper fiber batt further comprises applying pressure with the heat to form the paper fiber batt.
9. The method according to claim 6 , further comprising the step of encapsulating the paper fiber batt within a paper layer.
10. The method according to claim 9 , further comprising the step of connecting a first paper layer to a second paper layer to form the paper layer encapsulating the paper fiber batt.
11. A method of forming a shipping container comprising: mixing paper fibers with about 0.5% to 25% by weight meltable thermoplastic binder fiber to form a mixture; disposing the mixture onto a surface to form a layer of the mixture, the mixture having a density of 1300 to 1600 grams per square meter; applying heat to form a paper fiber batt from the mixture having a fixed width and fixed length; encapsulating the paper fiber batt within a paper layer; and folding the encapsulated paper fiber batt to form a bottom of the shipping container along the fold and also to define lateral edges adjacent to the bottom and a top arranged opposite to the bottom, the top defining an opening, wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%.
12. The method according to claim 11 , further comprising the step of sealing at least two lateral edges of the paper layer.
13. The method according to claim 12 , wherein the lateral edges are sealed by heat sealing.
14. The method according to claim 11 , wherein the step of encapsulating the paper fiber batt within the paper layer comprises securing a first paper layer to a second paper layer with the paper fiber batt located between the first paper layer and the second paper layer.
15. The method according to claim 11 , wherein the thermoplastic binder fibers make up less than 10% by weight of the paper fiber batt.
16. A method of forming a shipping container, the method comprising: mixing paper fibers with about 0.5% to 25% by weight meltable PE/PP bi-component binder fiber to form a mixture, the binder fibers being of a length of less than about 24 millimeters; applying heat to form a paper fiber ball from the mixture having a fixed width and fixed length; forming a shipping container from a paper medium, the shipping container defining an interior; securing a paper layer to the paper fiber batt; and surrounding the interior of the shipping container with the paper fiber batt, wherein subjecting the shipping container to a repulpability test produces a fiber yield of greater than 85%, wherein the repulpability test follows requirements set by Fibre Box Association of Elk Grove Village, Ill., and recited in Voluntary Standard For Repulping and Recycling Corrugated Fiberboard Treated to Improve Its Performance in the Presence of Water and Water Vapor as revised on Aug. 16, 2013.
17. The method of claim 16 , wherein the step of securing the paper layer to the paper fiber batt comprises encapsulating the paper fiber batt within the paper layer.
18. The method of claim 17 , wherein the step of forming the shipping container from the paper medium comprises folding the encapsulated paper fiber batt to form a bottom of the shipping container along the fold and also to define lateral edges adjacent to the bottom and a top arranged opposite to the bottom, the top defining an opening.
19. The method of claim 16 , wherein the thermoplastic binder fiber has a length of between about 0.5 mm to about 16 mm.
20. The method of claim 16 , wherein the step of forming the shipping container from the paper medium comprises forming a corrugated box, and wherein the step of securing the paper layer to the paper fiber batt comprises coupling the paper fiber batt to the corrugated box.
21. The method of claim 16 , wherein the PE/PP bi-component binder fiber makes up less than 10% by weight of the paper fiber batt.
22. The method of claim 16 , wherein about 50% of the PE/PP bi-component binder fiber has a length of about 1 millimeter and about 50% of the PE/PP bi-component binder fiber has a length of about 6 millimeters.
23. The method according to claim 6 , wherein the paper fiber batt has a thickness that is at least 1/16 inch.
The text of each claim as printed, for pasting a claim word for word. The links in the tree view name the same claims and elements.
Status
active
As of 2026-11-17, the USPTO record for US 11148870 shows no unresolved maintenance-fee lapse, and the term end computed from the dates in that record, leaving out a terminal disclaimer it shows without a date, is 2037-08-15 (20 years from the filing of a parent application on 2017-08-15), a date not yet passed; that disclaimer can only make the term end earlier (data version 20261117.2).
- Basis
- term_20y · terminal_disclaimer (20 years from the filing of a parent application on 2017-08-15, a terminal disclaimer on record without a date, which can only make the term end earlier than the date computed from the other dates)
- Term end
- 2037-08-15 Computed from the dates in the USPTO recordThis date leaves out a terminal disclaimer on record that has no date; that disclaimer can only make the term end earlier.
- Fee lapse
- none on record
- Reinstatement
- none on record; reinstatement_possible: false, not lapsed
- As of
- 2026-11-17
- Data version
- 20261117.2
A fact about the record with its basis and its as-of date, not legal advice.
Citations
References cited on the grant: 243 US patent documents · Cited by: 57 US patents in this data · Lists through the API: /api/v1/patent/us_patent_citation/11148870/ (needs a free key, as the links under Get this as data)
Family outside the US
Publications outside the US that Google Patents Public Datasets lists in the same patent family as US 11148870 (read 2026-10-15). Their legal status is not shown here.
| Office | Number | Kind | Published |
|---|---|---|---|
| AU | 2017359035 | A1 | 2019-05-30 |
| AU | 2017359035 | B2 | 2021-07-08 |
| AU | 2021204424 | A1 | 2021-07-29 |
| AU | 2021245201 | A1 | 2021-11-04 |
| AU | 2021204424 | B2 | 2023-04-06 |
| AU | 2023203006 | A1 | 2023-06-01 |
| AU | 2021245201 | B2 | 2023-12-21 |
| AU | 2024201654 | A1 | 2024-04-04 |
| AU | 2023203006 | B2 | 2025-11-27 |
| AU | 2026201502 | A1 | 2026-03-19 |
| AU | 2026202145 | A1 | 2026-04-09 |
| AU | 2024201654 | B2 | 2026-05-07 |
| CA | 3043192 | A1 | 2018-05-17 |
| CA | 3176052 | A1 | 2018-05-17 |
| CA | 3218319 | A1 | 2018-05-17 |
| CA | 3043192 | C | 2023-12-19 |
| CA | 3176052 | C | 2025-09-09 |
| CA | 3275549 | A1 | 2025-10-30 |
| CN | 110121579 | A | 2019-08-13 |
| CN | 113584941 | A | 2021-11-02 |
| CN | 113584941 | B | 2023-09-12 |
| CN | 117071332 | A | 2023-11-17 |
| CN | 121321436 | A | 2026-01-13 |
| CN | 117071332 | B | 2026-06-23 |
| EP | 3538708 | A1 | 2019-09-18 |
| EP | 3538708 | A4 | 2020-04-15 |
| EP | 3848505 | A1 | 2021-07-14 |
| EP | 3538708 | B1 | 2022-01-19 |
| EP | 3848505 | B1 | 2022-07-06 |
| EP | 4043639 | A1 | 2022-08-17 |
| EP | 3848505 | B8 | 2022-09-21 |
| EP | 4071298 | A1 | 2022-10-12 |
| EP | 4071298 | B1 | 2024-01-03 |
| EP | 4321681 | A2 | 2024-02-14 |
| EP | 4321681 | A3 | 2024-04-10 |
| EP | 4043639 | C0 | 2025-01-01 |
| EP | 4043639 | B1 | 2025-01-01 |
| EP | 4321681 | B1 | 2025-12-24 |
| MX | 2019005376 | A | 2019-10-02 |
| MX | 394653 | B | 2025-03-21 |
| WO | 2018089365 | A1 | 2018-05-17 |
This patent's family on USPTO Global Dossier
Family data from Google Patents Public Datasets, used under CC BY 4.0.
Record JSON
{
"patent_id": "11148870",
"status": "active",
"basis": [
"term_20y",
"terminal_disclaimer"
],
"reinstatement_possible": false,
"reinstatement_basis": "not lapsed",
"expiry_date_estimated": "2037-08-15",
"lapse_date": null,
"reinstated_date": null,
"as_of": "2026-11-17",
"data_version": "20261117.2",
"catalog_data_version": "20261117.2",
"permalink": "https://patentref.io/p/11148870?v=20261117.2",
"next_steps": [
{
"kind": "record",
"url": "https://patentref.io/p/11148870?v=20261117.2",
"audience": "human"
},
{
"kind": "patent",
"url": "https://patentref.io/api/v1/patent/11148870/",
"audience": "agent"
},
{
"kind": "fee_events",
"tool": "uspto_patent_center",
"url": "https://patentcenter.uspto.gov/applications?patentNumber=11148870",
"audience": "agent"
}
]
}
Get this as data
- Full record
/api/v1/patent/11148870/ - Status record
/api/v1/lapse/status/11148870/ - Claim tree
/api/v1/structure/claims/11148870/ - Brief
/api/v1/structure/brief/11148870/