US 11462722
Apparatuses and processes for forming a semi-solid electrode having high active solids loading and electrochemical cells including the same
Granted 2022-10-04 · Filed 2021-01-20 · Application 17/152,950 · Utility · Kind B2 · Prior publication US 2021/0226192 A1, 2021-07-22
- Assignee as printed
- 24M Technologies, Inc., Cambridge, MA (US)
- Kyocera Corporation, Kyoto (JP) · PatentsView label: KYOCERA Corporation
- Inventors
- Junji Aranami, Otsu (JP); Raymond ZAGARS, Quincy, MA (US); Naoki OTA, Lexington, MA (US); Junzheng CHEN, Concord, MA (US); Ricardo Bazzarella, Woburn, MA (US)
- CPC, current
- H01M4/0404; H01M4/0433; H01M4/043; H01M4/0435; H01M4/13; H01M4/624; Y02E60/10
Abstract
Embodiments described herein relate generally to apparatuses and processes for forming semi-solid electrodes having high active solids loading by removing excess electrolyte. In some embodiments, the semi-solid electrode material can be formed by mixing an active material and, optionally, a conductive material in a liquid electrolyte to form a suspension. In some embodiments, the semi-solid electrode material can be disposed onto a current collector to form an intermediate electrode. In some embodiments, the semi-solid electrode material can have a first composition in which the ratio of electrolyte to active material is between about 10:1 and about 1:1. In some embodiments, a method for converting the semi-solid electrode material from the first composition into the second composition includes removing a portion of the electrolyte from the semi-solid electrode material. In some embodiments, the method includes mechanically compressing the intermediate electrode to remove the portion of electrolyte from the semi-solid electrode material.
The claims as the USPTO long-text file prints them (text data version 20261117.3), split by PatentRef's claim parser (structure version 2): each claim's opening words, then one row for each element with its character offsets in the claim text, and the dependent claims under the claim they refer to. The split describes the text; it is not a reading of it. Each claim and each element has a link of its own. How the links are made.
Claim 1
Independent claim.
1. A method of forming a densified semi-solid electrode, the method comprising:
- Claim 1, element e1mixing an active material and a conductive material with a liquid electrolyte to form a semi-solid electrode material; 80–197
- Claim 1, element e2disposing the semi-solid electrode material onto a current collector; 199–267
- Claim 1, element e3disposing a semi-permeable membrane onto an exposed surface of the semi-solid electrode material; and 269–365
- Claim 1, element e4compressing the semi-solid electrode material between the current collector and the semi-permeable membrane to extract a portion of the liquid electrolyte and form the densified semi-solid electrode, 371–569
- Claim 1, element e5wherein the densified semi-solid electrode includes between about 60% and about 85% by volume of an active material.571–686
10 dependent claims: 2 to 11 (2, 3, 4, 5, 6, 7, 8, 9, 10, 11 on claim 1)
Claim 2
Depends on claim 1.
2. The method of claim 1, wherein
- Claim 2, element e1the semi-permeable membrane is configured to absorb the portion of the liquid electrolyte extracted during compressing.34–152
Claim 3
Depends on claim 1.
3. The method of claim 1, further comprising:
- Claim 3, element e1disposing an absorptive material onto an exposed surface of the semi-permeable membrane, the absorptive material configured to absorb the portion of the liquid electrolyte extracted during compressing.46–246
Claim 4
Depends on claim 1.
4. The method of claim 1, wherein
- Claim 4, element e1mechanically compressing the semi-solid electrode material includes compressing the semi-solid material between a die and a base.34–162
Claim 5
Depends on claim 1.
5. The method of claim 1, wherein
- Claim 5, element e1the compressed semi-solid electrode material includes greater than about 70 wt % of the active material.34–137
Claim 6
Depends on claim 1.
6. The method of claim 1, wherein
- Claim 6, element e1the semi-solid electrode material after mixing has a first composition in which the liquid electrolyte is between about 50 wt % and about 80 wt % of the semi-solid electrode material, and wherein the semi-solid electrode material after compressing has a second composition in which the liquid electrolyte is between about 10 wt % and about 45 wt % of the semi-solid electrode material.34–418
Claim 7
Depends on claim 1.
7. The method of claim 1, wherein
- Claim 7, element e1the semi-solid electrode material after mixing has a first ratio of liquid electrolyte to active material of between about 10:1 and about 1:1; and 34–175
- Claim 7, element e2wherein the semi-solid electrode material after compressing has a second ratio of liquid electrolyte to active material of between about 5:1 and about 1:3.181–335
Claim 8
Depends on claim 1.
8. The method of claim 1, wherein
- Claim 8, element e1the semi-solid electrode material after mixing has a first active material molarity of between about 5M and about 15M; and 34–151
- Claim 8, element e2wherein the semi-solid electrode material after compressing has a second active material molarity of between about 16M and about 24M.157–289
Claim 9
Depends on claim 1.
9. The method of claim 1, wherein
- Claim 9, element e1the semi-solid electrode material after mixing has a first energy density of between about 3 mAh/g and about 5 mAh/g; and 34–150
- Claim 9, element e2wherein the semi-solid electrode material after compressing has a second energy density of between about 6 mAh/g and about 14 mAh/g.156–287
Claim 10
Depends on claim 1.
10. The method of claim 1, wherein
- Claim 10, element e1the conductive material includes conductive particles.35–88
Claim 11
Depends on claim 1.
11. The method of claim 1, wherein
- Claim 11, element e1the densified semi-solid electrode is a first electrode and the current collector is a first current collector, further comprising: 35–165
- Claim 11, element e2removing the semi-permeable membrane from the first electrode; 167–228
- Claim 11, element e3placing a second electrode on a second current collector; 230–286
- Claim 11, element e4placing a separator on the second electrode, such that a first surface of the separator contacts the second electrode and a second surface of the separator is exposed, the second surface opposite the first surface; 288–501
- Claim 11, element e5placing droplets of electrolyte on the second surface of the separator; and 503–573
- Claim 11, element e6placing the first electrode on the separator to form an electrochemical cell.579–655
Claim 12
Independent claim.
12. A method, comprising:
- Claim 12, element e1mixing an active material and a conductive material with a liquid electrolyte to form a semi-solid electrode material having a first volume; 26–165
- Claim 12, element e2interposing the semi-solid electrode material between a current collector and a semi-permeable membrane; and 167–270
- Claim 12, element e3applying a compressive force to the semi-solid electrode material via a roller such that the semi-solid electrode material has a second volume less than the first volume.276–445
6 dependent claims: 13 to 18 (13, 16 on claim 12; 14 on 13; 15 on 14; 17, 18 on 16)
Claim 13
Depends on claim 12.
13. The method of claim 12, further comprising:
- Claim 13, element e1exposing the semi-solid electrode material to an absorptive material, such that a portion of the liquid electrolyte migrates from the semi-solid electrode material to the absorptive material.48–238
Claim 14
Depends on claim 13.
14. The method of claim 13, wherein
- Claim 14, element e1the absorptive material is conveyed by one or more rollers.36–94
Claim 15
Depends on claim 14.
15. The method of claim 14, wherein
- Claim 15, element e1a flat portion of the absorptive material is in contact with the semi-solid electrode material.36–130
Claim 16
Depends on claim 12.
16. The method of claim 12, wherein
- Claim 16, element e1the second volume is between about 50% and about 95% of the first volume.36–108
Claim 17
Depends on claim 16.
17. The method of claim 16, wherein
- Claim 17, element e1the second volume is between about 50% and about 80% of the first volume.36–108
Claim 18
Depends on claim 16.
18. The method of claim 16, wherein
- Claim 18, element e1the second volume is between about 70% and about 95% of the first volume.36–108
Claim 19
Independent claim.
19. A method, comprising:
- Claim 19, element e1mixing an active material and a conductive material with a liquid electrolyte to form a semi-solid electrode material having a first thickness; 26–168
- Claim 19, element e2interposing the semi-solid electrode material between a current collector and a semi-permeable membrane; and 170–273
- Claim 19, element e3applying a compressive force to the semi-solid electrode material via a roller such that the semi-solid electrode material has a second thickness less than the first thickness.279–454
3 dependent claims: 20 to 22 (20, 21, 22 on claim 19)
Claim 20
Depends on claim 19.
20. The method of claim 19, wherein
- Claim 20, element e1the first thickness is between about 100 μm and about 2,000 μm.36–98
Claim 21
Depends on claim 19.
21. The method of claim 19, wherein
- Claim 21, element e1the second thickness is between about 5 μm and about 50 μm.36–94
Claim 22
Depends on claim 19.
22. The method of claim 19, wherein
- Claim 22, element e1mechanically compressing is accomplished by mechanically compressing the semi-solid electrode material between a base and a die of a mechanical press.36–185
Claim 23
Independent claim.
23. A method, comprising:
- Claim 23, element e1mixing an active material and a conductive material with a liquid electrolyte to form a first semi-solid electrode material having a first composition comprising between about 50 wt % and about 80 wt % of the liquid electrolyte; 26–253
- Claim 23, element e2interposing the first semi-solid electrode material between a current collector and a semi-permeable membrane; and 255–364
- Claim 23, element e3mechanically compressing the first semi-solid electrode material to form a second semi-solid electrode material having a second composition comprising between about 10 wt % and about 45 wt % of the liquid electrolyte.370–586
Claim 24
Independent claim.
24. A method, comprising:
- Claim 24, element e1mixing an active material and a conductive material with a liquid electrolyte to form a first semi-solid electrode material having a first density; 26–172
- Claim 24, element e2interposing the first semi-solid electrode material between a current collector and a semi-permeable membrane; and 174–283
- Claim 24, element e3mechanically compressing the first semi-solid electrode material to form a second semi-solid electrode material having a second density greater than the first density, the second semi-solid electrode material including between about 60% and about 85% by volume of the active material.289–572
6 dependent claims: 25 to 30 (25 on claim 24; 26 on 25; 27 on 26; 28 on 27; 29 on 28; 30 on 29)
Claim 25
Depends on claim 24.
25. The method of claim 24, wherein
- Claim 25, element e1the first density is less than about 2 g/cm3.36–80
Claim 26
Depends on claim 25.
26. The method of claim 25, wherein
- Claim 26, element e1the second density is between about 2.1 g/cm3 and about 4 g/cm3.36–99
Claim 27
Depends on claim 26.
27. The method of claim 26, wherein
- Claim 27, element e1an energy density of the second semi-solid electrode material is greater than about 7 mAh/g.36–127
Claim 28
Depends on claim 27.
28. The method of claim 27, wherein
- Claim 28, element e1the energy density of the second semi-solid electrode material is greater than about 8 mAh/g.36–128
Claim 29
Depends on claim 28.
29. The method of claim 28, wherein
- Claim 29, element e1the energy density of the second semi-solid electrode material is greater than about 9 mAh/g.36–128
Claim 30
Depends on claim 29.
30. The method of claim 29, wherein
- Claim 30, element e1the energy density of the second semi-solid electrode material is greater than about 10 mAh/g.36–129
1. A method of forming a densified semi-solid electrode, the method comprising: mixing an active material and a conductive material with a liquid electrolyte to form a semi-solid electrode material; disposing the semi-solid electrode material onto a current collector; disposing a semi-permeable membrane onto an exposed surface of the semi-solid electrode material; and compressing the semi-solid electrode material between the current collector and the semi-permeable membrane to extract a portion of the liquid electrolyte and form the densified semi-solid electrode, wherein the densified semi-solid electrode includes between about 60% and about 85% by volume of an active material.
2. The method of claim 1, wherein the semi-permeable membrane is configured to absorb the portion of the liquid electrolyte extracted during compressing.
3. The method of claim 1, further comprising: disposing an absorptive material onto an exposed surface of the semi-permeable membrane, the absorptive material configured to absorb the portion of the liquid electrolyte extracted during compressing.
4. The method of claim 1, wherein mechanically compressing the semi-solid electrode material includes compressing the semi-solid material between a die and a base.
5. The method of claim 1, wherein the compressed semi-solid electrode material includes greater than about 70 wt % of the active material.
6. The method of claim 1, wherein the semi-solid electrode material after mixing has a first composition in which the liquid electrolyte is between about 50 wt % and about 80 wt % of the semi-solid electrode material, and wherein the semi-solid electrode material after compressing has a second composition in which the liquid electrolyte is between about 10 wt % and about 45 wt % of the semi-solid electrode material.
7. The method of claim 1, wherein the semi-solid electrode material after mixing has a first ratio of liquid electrolyte to active material of between about 10:1 and about 1:1; and wherein the semi-solid electrode material after compressing has a second ratio of liquid electrolyte to active material of between about 5:1 and about 1:3.
8. The method of claim 1, wherein the semi-solid electrode material after mixing has a first active material molarity of between about 5M and about 15M; and wherein the semi-solid electrode material after compressing has a second active material molarity of between about 16M and about 24M.
9. The method of claim 1, wherein the semi-solid electrode material after mixing has a first energy density of between about 3 mAh/g and about 5 mAh/g; and wherein the semi-solid electrode material after compressing has a second energy density of between about 6 mAh/g and about 14 mAh/g.
10. The method of claim 1, wherein the conductive material includes conductive particles.
11. The method of claim 1, wherein the densified semi-solid electrode is a first electrode and the current collector is a first current collector, further comprising: removing the semi-permeable membrane from the first electrode; placing a second electrode on a second current collector; placing a separator on the second electrode, such that a first surface of the separator contacts the second electrode and a second surface of the separator is exposed, the second surface opposite the first surface; placing droplets of electrolyte on the second surface of the separator; and placing the first electrode on the separator to form an electrochemical cell.
12. A method, comprising: mixing an active material and a conductive material with a liquid electrolyte to form a semi-solid electrode material having a first volume; interposing the semi-solid electrode material between a current collector and a semi-permeable membrane; and applying a compressive force to the semi-solid electrode material via a roller such that the semi-solid electrode material has a second volume less than the first volume.
13. The method of claim 12, further comprising: exposing the semi-solid electrode material to an absorptive material, such that a portion of the liquid electrolyte migrates from the semi-solid electrode material to the absorptive material.
14. The method of claim 13, wherein the absorptive material is conveyed by one or more rollers.
15. The method of claim 14, wherein a flat portion of the absorptive material is in contact with the semi-solid electrode material.
16. The method of claim 12, wherein the second volume is between about 50% and about 95% of the first volume.
17. The method of claim 16, wherein the second volume is between about 50% and about 80% of the first volume.
18. The method of claim 16, wherein the second volume is between about 70% and about 95% of the first volume.
19. A method, comprising: mixing an active material and a conductive material with a liquid electrolyte to form a semi-solid electrode material having a first thickness; interposing the semi-solid electrode material between a current collector and a semi-permeable membrane; and applying a compressive force to the semi-solid electrode material via a roller such that the semi-solid electrode material has a second thickness less than the first thickness.
20. The method of claim 19, wherein the first thickness is between about 100 μm and about 2,000 μm.
21. The method of claim 19, wherein the second thickness is between about 5 μm and about 50 μm.
22. The method of claim 19, wherein mechanically compressing is accomplished by mechanically compressing the semi-solid electrode material between a base and a die of a mechanical press.
23. A method, comprising: mixing an active material and a conductive material with a liquid electrolyte to form a first semi-solid electrode material having a first composition comprising between about 50 wt % and about 80 wt % of the liquid electrolyte; interposing the first semi-solid electrode material between a current collector and a semi-permeable membrane; and mechanically compressing the first semi-solid electrode material to form a second semi-solid electrode material having a second composition comprising between about 10 wt % and about 45 wt % of the liquid electrolyte.
24. A method, comprising: mixing an active material and a conductive material with a liquid electrolyte to form a first semi-solid electrode material having a first density; interposing the first semi-solid electrode material between a current collector and a semi-permeable membrane; and mechanically compressing the first semi-solid electrode material to form a second semi-solid electrode material having a second density greater than the first density, the second semi-solid electrode material including between about 60% and about 85% by volume of the active material.
25. The method of claim 24, wherein the first density is less than about 2 g/cm3.
26. The method of claim 25, wherein the second density is between about 2.1 g/cm3 and about 4 g/cm3.
27. The method of claim 26, wherein an energy density of the second semi-solid electrode material is greater than about 7 mAh/g.
28. The method of claim 27, wherein the energy density of the second semi-solid electrode material is greater than about 8 mAh/g.
29. The method of claim 28, wherein the energy density of the second semi-solid electrode material is greater than about 9 mAh/g.
30. The method of claim 29, wherein the energy density of the second semi-solid electrode material is greater than about 10 mAh/g.
The text of each claim as printed, for pasting a claim word for word. The links in the tree view name the same claims and elements.
Status
active
As of 2026-11-17, the USPTO record for US 11462722 shows no unresolved maintenance-fee lapse, and the term end computed from the dates in that record is 2041-03-28 (20 years from filing, plus 67 days of patent term adjustment), a date not yet passed (data version 20261117.2).
- Basis
- term_20y · pta_days:67 (20 years from filing, plus 67 days of patent term adjustment)
- Term end
- 2041-03-28 Computed from the dates in the USPTO record
- Fee lapse
- none on record
- Reinstatement
- none on record; reinstatement_possible: false, not lapsed
- As of
- 2026-11-17
- Data version
- 20261117.2
A fact about the record with its basis and its as-of date, not legal advice.
Citations
References cited on the grant: 52 US patent documents · Cited by: 46 US patents in this data · Lists through the API: /api/v1/patent/us_patent_citation/11462722/ (needs a free key, as the links under Get this as data)
Family outside the US
Publications outside the US that Google Patents Public Datasets lists in the same patent family as US 11462722 (read 2026-10-15). Their legal status is not shown here.
| Office | Number | Kind | Published |
|---|---|---|---|
| CN | 115244729 | A | 2022-10-25 |
| CN | 115244729 | B | 2026-04-10 |
| EP | 4094309 | A1 | 2022-11-30 |
| JP | 2023511559 | A | 2023-03-20 |
| JP | 7721541 | B2 | 2025-08-12 |
| JP | 2025172746 | A | 2025-11-26 |
| WO | 2021150602 | A1 | 2021-07-29 |
This patent's family on USPTO Global Dossier
Family data from Google Patents Public Datasets, used under CC BY 4.0.
Record JSON
{
"patent_id": "11462722",
"status": "active",
"basis": [
"term_20y",
"pta_days:67"
],
"reinstatement_possible": false,
"reinstatement_basis": "not lapsed",
"expiry_date_estimated": "2041-03-28",
"lapse_date": null,
"reinstated_date": null,
"as_of": "2026-11-17",
"data_version": "20261117.2",
"catalog_data_version": "20261117.2",
"permalink": "https://patentref.io/p/11462722?v=20261117.2",
"next_steps": [
{
"kind": "record",
"url": "https://patentref.io/p/11462722?v=20261117.2",
"audience": "human"
},
{
"kind": "patent",
"url": "https://patentref.io/api/v1/patent/11462722/",
"audience": "agent"
},
{
"kind": "fee_events",
"tool": "uspto_patent_center",
"url": "https://patentcenter.uspto.gov/applications?patentNumber=11462722",
"audience": "agent"
}
]
}
Get this as data
- Full record
/api/v1/patent/11462722/ - Status record
/api/v1/lapse/status/11462722/ - Claim tree
/api/v1/structure/claims/11462722/ - Brief
/api/v1/structure/brief/11462722/
These four links need a free key (1,000 requests a month). Opened in a browser, which sends no key, they answer 403. Get a free key on the sign-up page, then send it in the X-Api-Key header. To see the shape of an answer without a key, open Try it.